Process for Vanadium Extraction from Vanadium Ore in West of Hunan Province

Liu Zhen-na

Open publisher page 0 citations

Abstract

Recovery of vanadium pentoxide from stone coal vanadium ore in west of Hunan province has been studied. The influence of percentage of additives,roasting temperature,roasting time,particle size of the ore,sulfuric acid volume,leaching temperature and leaching time on leaching rate was investigated. The experimental results showed that with the vanadium ore particle size of- 74 μm more than 71%,the stone coal was roasted at 870 ℃ for 4 h without additives,the leaching rate of vanadium can be more than 87% after the obtained calcine was leached at 25 ℃ for 1h in a solution with sulfuric acid dosage of 1%. V 2 O 5 was recovered from the leach solution of vanadium by the technology of resin absorption-vanadium precipitation-calcination,with main technical indicators all reaching standards( YB / T5304- 2006) for metallurgy 99. Vanadium overall recovery was 84. 5%.

About this research paper

What this paper is about

Recovery of vanadium pentoxide from stone coal vanadium ore in west of Hunan province has been studied. The influence of percentage of additives,roasting temperature,roasting time,particle size of the ore,sulfuric acid volume,leaching temperature and leaching time on leaching rate was investigated. The experimental results showed that with the vanadium ore particle size of- 74 μm more than 71%,the stone coal was roasted at 870 ℃ for 4 h without additives,the leaching rate of vanadium can be more than 87% after the obtained calcine was leached at 25 ℃ for 1h in a solution with sulfuric acid dosage of 1%. V 2 O 5 was recovered from the leach solution of vanadium by the technology of resin absorption-vanadium precipitation-calcination,with main technical indicators all reaching standards( YB / T5304- 2006) for metallurgy 99. Vanadium overall recovery was 84. 5%.

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Recovery of vanadium pentoxide from stone coal vanadium ore in west of Hunan province has been studied. The influence of percentage of additives,roasting temperature,roasting time,particle size of the ore,sulfuric acid volume,leaching temperature and leaching time on leaching rate was investigated. The experimental results showed that with the vanadium ore particle size of- 74 μm more than 71%,the stone coal was roasted at 870 ℃ for 4 h without additives,the leaching rate of vanadium can be more than 87% after the obtained calcine was leached at 25 ℃ for 1h in a solution with sulfuric acid dosage of 1%. V 2 O 5 was recovered from the leach solution of vanadium by the technology of resin absorption-vanadium precipitation-calcination,with main technical indicators all reaching standards( YB / T5304- 2006) for metallurgy 99. Vanadium overall recovery was 84. 5%.

Key concepts: Vanadium, Roasting, Leaching (pedology), Sulfuric acid, Pentoxide, Metallurgy, Calcination, Coal