Study on Leaching of Vanadium From Silicate-type Vanadium Ore
Qian Shi
Abstract
Qian Shi
Abstract
Leaching of Vanadium from silicate-type vanadium ore has been research by roasting and leaching using acid.The optimal conditions were determined that roasting temperature was 800 ℃,roasting time was 3 h,ore granularity was 80% for 0.074 mm diameter granule.Leaching rate of vanadium was up to 85 % at the conditions of leaching temperature of 70℃ and leaching time of 0.5h.
OpenAlex reports 1 citations for this work. Citation counts describe recorded attention and do not establish research quality.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
Leaching of Vanadium from silicate-type vanadium ore has been research by roasting and leaching using acid.The optimal conditions were determined that roasting temperature was 800 ℃,roasting time was 3 h,ore granularity was 80% for 0.074 mm diameter granule.Leaching rate of vanadium was up to 85 % at the conditions of leaching temperature of 70℃ and leaching time of 0.5h.
Key concepts: Vanadium, Leaching (pedology), Roasting, Silicate, Metallurgy, Chemistry, Materials science, Geology