2011Mining and Metallurgical EngineeringRequires access

Process for Vanadium Extraction from Vanadium-bearing Stone Coal

Zhou Zai-xing

Open publisher page 0 citations

Abstract

According to the characteristics of the vanadium-bearing stone-coal in West of Hunan Province,a roasting-acid leaching technology by adding X as additives was adopted for extracting vanadium from stone coal.The influence of percentage of additives,roasting temperature,roasting time,sulfuric acid volume,leaching temperature and leaching time upon leaching rate was investigated.The experimental results showed that while the stone coal was roasted at 750 ℃ for 2 h with the dosage of additive X being 9%,the leaching rate of vanadium can be more than 95% after the obtained calcine was leached at 50 ℃ for 4 h in a solution with sulfuric acid dosage of 2%.V2O5 was recovered from the leach solution of vanadium by the technology of resin absorption-vanadium precipitation-calcination,with main technical indicators all reaching standards(GB3283-87) for chemical vanadium powder.

About this research paper

What this paper is about

According to the characteristics of the vanadium-bearing stone-coal in West of Hunan Province,a roasting-acid leaching technology by adding X as additives was adopted for extracting vanadium from stone coal.The influence of percentage of additives,roasting temperature,roasting time,sulfuric acid volume,leaching temperature and leaching time upon leaching rate was investigated.The experimental results showed that while the stone coal was roasted at 750 ℃ for 2 h with the dosage of additive X being 9%,the leaching rate of vanadium can be more than 95% after the obtained calcine was leached at 50 ℃ for 4 h in a solution with sulfuric acid dosage of 2%.V2O5 was recovered from the leach solution of vanadium by the technology of resin absorption-vanadium precipitation-calcination,with main technical indicators all reaching standards(GB3283-87) for chemical vanadium powder.

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

According to the characteristics of the vanadium-bearing stone-coal in West of Hunan Province,a roasting-acid leaching technology by adding X as additives was adopted for extracting vanadium from stone coal.The influence of percentage of additives,roasting temperature,roasting time,sulfuric acid volume,leaching temperature and leaching time upon leaching rate was investigated.The experimental results showed that while the stone coal was roasted at 750 ℃ for 2 h with the dosage of additive X being 9%,the leaching rate of vanadium can be more than 95% after the obtained calcine was leached at 50 ℃ for 4 h in a solution with sulfuric acid dosage of 2%.V2O5 was recovered from the leach solution of vanadium by the technology of resin absorption-vanadium precipitation-calcination,with main technical indicators all reaching standards(GB3283-87) for chemical vanadium powder.

Key concepts: Vanadium, Roasting, Leaching (pedology), Sulfuric acid, Coal, Calcination, Metallurgy, Materials science