Abstract

In order to resolve the problems of ultra-low head slab caster like tundish small capacity,short retain time in tundish,unreasonable flow field,uneasy removing of inclusion,secondary oxidation heavy,through taking the methods like the tundish expanding capacity reconstruction,optimizing the flow field of tundish,the applying of continuous temperature measurement,nano-fibers insulation blank technique and the fining slag of tudish technology and so on,the aim of inclusion removing was reached.The total oxygen contain in steel was decreased by 20.5×10-6 averagely and the average temperature drop in the tundish was reduced by 3.3 ℃.

About this research paper

What this paper is about

In order to resolve the problems of ultra-low head slab caster like tundish small capacity,short retain time in tundish,unreasonable flow field,uneasy removing of inclusion,secondary oxidation heavy,through taking the methods like the tundish expanding capacity reconstruction,optimizing the flow field of tundish,the applying of continuous temperature measurement,nano-fibers insulation blank technique and the fining slag of tudish technology and so on,the aim of inclusion removing was reached.The total oxygen contain in steel was decreased by 20.5×10-6 averagely and the average temperature drop in the tundish was reduced by 3.3 ℃.

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

In order to resolve the problems of ultra-low head slab caster like tundish small capacity,short retain time in tundish,unreasonable flow field,uneasy removing of inclusion,secondary oxidation heavy,through taking the methods like the tundish expanding capacity reconstruction,optimizing the flow field of tundish,the applying of continuous temperature measurement,nano-fibers insulation blank technique and the fining slag of tudish technology and so on,the aim of inclusion removing was reached.The total oxygen contain in steel was decreased by 20.5×10-6 averagely and the average temperature drop in the tundish was reduced by 3.3 ℃.

Key concepts: Tundish, Caster, Slab, Metallurgy, Continuous casting, Ladle, Materials science, Head (geology)

Related papers

Back to paper searchBrowse research topicsOriginal source
Application of Tudish Metallurgical Technology in Jinan Steel's Ultra-low Head Slab Caster — Research Paper | ScholarLens