2009•Dyeing & FinishingRequires access

DP finish of all cotton poplin

Guo Zhi-hui

Open publisher page 0 citations

Abstract

DP finish of all cotton poplin was carried out,factors exerting influence on crease resistance were analyzed,such as resin dosage,curing temperature,pH value and chemicals.Optimum conditions were defined as follows: resin MS-08 200 g/L,catalyst WS-08 30 g/L,softener SIO 20 g/L,fiber protector DT-6500 40 g/L,penetrator XC-J 1 g/L,pH value of finishing liquor 4.5,curing at 125 ℃ for 3 minutes.Bulk production demostrated that cotton fabric after treatment featured good properties of above 3-level DP value,200 N breaking strength,6 N tearing strength,as well as formaldehyde content lower than 75 mg/kg.

About this research paper

What this paper is about

DP finish of all cotton poplin was carried out,factors exerting influence on crease resistance were analyzed,such as resin dosage,curing temperature,pH value and chemicals.Optimum conditions were defined as follows: resin MS-08 200 g/L,catalyst WS-08 30 g/L,softener SIO 20 g/L,fiber protector DT-6500 40 g/L,penetrator XC-J 1 g/L,pH value of finishing liquor 4.5,curing at 125 ℃ for 3 minutes.Bulk production demostrated that cotton fabric after treatment featured good properties of above 3-level DP value,200 N breaking strength,6 N tearing strength,as well as formaldehyde content lower than 75 mg/kg.

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

DP finish of all cotton poplin was carried out,factors exerting influence on crease resistance were analyzed,such as resin dosage,curing temperature,pH value and chemicals.Optimum conditions were defined as follows: resin MS-08 200 g/L,catalyst WS-08 30 g/L,softener SIO 20 g/L,fiber protector DT-6500 40 g/L,penetrator XC-J 1 g/L,pH value of finishing liquor 4.5,curing at 125 ℃ for 3 minutes.Bulk production demostrated that cotton fabric after treatment featured good properties of above 3-level DP value,200 N breaking strength,6 N tearing strength,as well as formaldehyde content lower than 75 mg/kg.

Key concepts: Curing (chemistry), Formaldehyde, Tearing, Composite material, Breaking strength, Materials science, Chemistry, Organic chemistry