Based on the statistic data of breakout of bloom continuous caster in No.2 Steelmaking and Rolling Plant of Tang Steel in 2008,main characteristics and mechanism of breakout caused by slag entrapment,sticking and longitudinal corner crack are analyzed.The main causes of the breakout are related to the following factors: the performance of mold powder,accuracy of mold,extent of hot metal overheat,casting speed,alignment of the submerged entry nozzle with the mold as well as casting operations.By means of corresponding measures being taken,the breakout rate of caster was remarkably decreased.

About this research paper

What this paper is about

Based on the statistic data of breakout of bloom continuous caster in No.2 Steelmaking and Rolling Plant of Tang Steel in 2008,main characteristics and mechanism of breakout caused by slag entrapment,sticking and longitudinal corner crack are analyzed.The main causes of the breakout are related to the following factors: the performance of mold powder,accuracy of mold,extent of hot metal overheat,casting speed,alignment of the submerged entry nozzle with the mold as well as casting operations.By means of corresponding measures being taken,the breakout rate of caster was remarkably decreased.

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Based on the statistic data of breakout of bloom continuous caster in No.2 Steelmaking and Rolling Plant of Tang Steel in 2008,main characteristics and mechanism of breakout caused by slag entrapment,sticking and longitudinal corner crack are analyzed.The main causes of the breakout are related to the following factors: the performance of mold powder,accuracy of mold,extent of hot metal overheat,casting speed,alignment of the submerged entry nozzle with the mold as well as casting operations.By means of corresponding measures being taken,the breakout rate of caster was remarkably decreased.

Key concepts: Breakout, Caster, Nozzle, Ladle, Mold, Continuous casting, Metallurgy, Materials science

Related papers

Back to paper searchBrowse research topicsOriginal source
Analysis on breakout of bloom continuous caster and its countermeasures — Research Paper | ScholarLens