2009SteelmakingRequires access

Analysis on breakout of bloom continuous caster and countermeasures

Zhao Zhongfu

Open publisher page 1 citations

Abstract

The statistics of breakout of the bloom continuous caster in No.1 steelmaking plant of WISCO in 2006 have been made and the main characteristics and mechanism of sticking breakout and longitudinal corner crack induced breakout analyzed.The main causes to the above mentioned breakouts are found to be such a few factors as the performance of mold powder,accuracy of mold,extent of hot metal overheat,casting speed,and alignment of the submerged entry nozzle with the mold and etc,and thereupon certain countermeasures have been taken up.As the results,the breakout rate of caster is decreased remarkably.

About this research paper

What this paper is about

The statistics of breakout of the bloom continuous caster in No.1 steelmaking plant of WISCO in 2006 have been made and the main characteristics and mechanism of sticking breakout and longitudinal corner crack induced breakout analyzed.The main causes to the above mentioned breakouts are found to be such a few factors as the performance of mold powder,accuracy of mold,extent of hot metal overheat,casting speed,and alignment of the submerged entry nozzle with the mold and etc,and thereupon certain countermeasures have been taken up.As the results,the breakout rate of caster is decreased remarkably.

Why it matters

OpenAlex reports 1 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

The statistics of breakout of the bloom continuous caster in No.1 steelmaking plant of WISCO in 2006 have been made and the main characteristics and mechanism of sticking breakout and longitudinal corner crack induced breakout analyzed.The main causes to the above mentioned breakouts are found to be such a few factors as the performance of mold powder,accuracy of mold,extent of hot metal overheat,casting speed,and alignment of the submerged entry nozzle with the mold and etc,and thereupon certain countermeasures have been taken up.As the results,the breakout rate of caster is decreased remarkably.

Key concepts: Breakout, Caster, Nozzle, Mold, Ladle, Continuous casting, Bloom, Metallurgy