Calcified roasting-acid leaching process of vanadium from low-grade vanadium-containing stone coal

Wang Taiyin

Open publisher page 0 citations

Abstract

The low-grade vanadium-containing stone coal used in this experiment was collected from Wuxi Country, Chongqing City, China. The experiment focused on the vanadium recovery from roasted residue through optimizing the process conditions of an effective and environmentally-friendly technology, named calcified roasting-sulfuric acid leaching technology. By single-factor experiments and orthogonal experiments, the effects of roasting temperature, roasting time, sulfuric acid concentration and leaching time on the leaching ratio of vanadium were analyzed. The results showed that the leaching ratio of vanadium reached 85.5% under the proper technological conditions of roasting temperature=950℃, roasting time=4 h, 40% concentration of sulfuric acid and leaching time=6 h.

About this research paper

What this paper is about

The low-grade vanadium-containing stone coal used in this experiment was collected from Wuxi Country, Chongqing City, China. The experiment focused on the vanadium recovery from roasted residue through optimizing the process conditions of an effective and environmentally-friendly technology, named calcified roasting-sulfuric acid leaching technology. By single-factor experiments and orthogonal experiments, the effects of roasting temperature, roasting time, sulfuric acid concentration and leaching time on the leaching ratio of vanadium were analyzed. The results showed that the leaching ratio of vanadium reached 85.5% under the proper technological conditions of roasting temperature=950℃, roasting time=4 h, 40% concentration of sulfuric acid and leaching time=6 h.

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

The low-grade vanadium-containing stone coal used in this experiment was collected from Wuxi Country, Chongqing City, China. The experiment focused on the vanadium recovery from roasted residue through optimizing the process conditions of an effective and environmentally-friendly technology, named calcified roasting-sulfuric acid leaching technology. By single-factor experiments and orthogonal experiments, the effects of roasting temperature, roasting time, sulfuric acid concentration and leaching time on the leaching ratio of vanadium were analyzed. The results showed that the leaching ratio of vanadium reached 85.5% under the proper technological conditions of roasting temperature=950℃, roasting time=4 h, 40% concentration of sulfuric acid and leaching time=6 h.

Key concepts: Roasting, Vanadium, Sulfuric acid, Leaching (pedology), Coal, Metallurgy, Chemistry, Materials science

Related papers

Back to paper searchBrowse research topicsOriginal source
Calcified roasting-acid leaching process of vanadium from low-grade vanadium-containing stone coal — Research Paper | ScholarLens