A laboratory electric rotary kiln was used in the dynamic oxidizing roasting of Hubei stone coal.The results showed that the optimum roasting conditions are as follows: charge ratio of 16%,roasting temperature of 800 ℃,roasting time of 2.5 h and NaCl dosage of 10%.Compared with the static roasting with Muffle furnace,the dynamic oxidizing roasting can dramatically reduce NaCl dosage from 18% to 10% and the roasting temperature from 850 ℃ to 800 ℃,and distinctly raise the leaching rate from 64.03% to 72.64%.

About this research paper

What this paper is about

A laboratory electric rotary kiln was used in the dynamic oxidizing roasting of Hubei stone coal.The results showed that the optimum roasting conditions are as follows: charge ratio of 16%,roasting temperature of 800 ℃,roasting time of 2.5 h and NaCl dosage of 10%.Compared with the static roasting with Muffle furnace,the dynamic oxidizing roasting can dramatically reduce NaCl dosage from 18% to 10% and the roasting temperature from 850 ℃ to 800 ℃,and distinctly raise the leaching rate from 64.03% to 72.64%.

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

A laboratory electric rotary kiln was used in the dynamic oxidizing roasting of Hubei stone coal.The results showed that the optimum roasting conditions are as follows: charge ratio of 16%,roasting temperature of 800 ℃,roasting time of 2.5 h and NaCl dosage of 10%.Compared with the static roasting with Muffle furnace,the dynamic oxidizing roasting can dramatically reduce NaCl dosage from 18% to 10% and the roasting temperature from 850 ℃ to 800 ℃,and distinctly raise the leaching rate from 64.03% to 72.64%.

Key concepts: Roasting, Oxidizing agent, Rotary kiln, Coal, Metallurgy, Vanadium, Muffle furnace, Leaching (pedology)

Related papers

Back to paper searchBrowse research topicsOriginal source
Extraction of Vanadium from Stone Coal by Dynamic Oxidizing Roasting Process with Laboratory Electric Rotary Kiln — Research Paper | ScholarLens