2015AIP AdvancesOpen access

Comparative study on the charge-trapping properties of TaAlO and ZrAlO high-k composites with designed band alignment

W. Lu, Chao-Gang Wei, K. Jiang, Jiefeng Liu, Jian‐Xin Lu, Ping Han, A. D. Li, Yidong Xia, Bin Xu, J. Yin, Z. G. Liu

Open full text 3 citations

Abstract

The charge-trapping memory (CTM) structures Pt/Al2O3/TaAlO/Al2O3/p-Si and Pt/Al2O3/ZrAlO/Al2O3/p-Si were fabricated by using rf-sputtering and atomic layer deposition techniques, in which the potentials at the bottom of the conduction band (PBCB) of high-k composites TaAlO and ZrAlO were specially designed. With a lower PBCB difference between TaAlO and p-Si than that between ZrAlO and p-Si, TaAlO CTM device shows a better charge-trapping performance. A density of trapped charges 2.88 × 1013/cm2 at an applied voltage of ±7 V was obtained for TaAlO CTM device, and it could keep about 60% of initially trapped charges after 10 years. It was suggested that the PBCB difference between high-k composite and p-Si dominates their charge-trapping behaviors.

About this research paper

What this paper is about

The charge-trapping memory (CTM) structures Pt/Al2O3/TaAlO/Al2O3/p-Si and Pt/Al2O3/ZrAlO/Al2O3/p-Si were fabricated by using rf-sputtering and atomic layer deposition techniques, in which the potentials at the bottom of the conduction band (PBCB) of high-k composites TaAlO and ZrAlO were specially designed. With a lower PBCB difference between TaAlO and p-Si than that between ZrAlO and p-Si, TaAlO CTM device shows a better charge-trapping performance. A density of trapped charges 2.88 × 1013/cm2 at an applied voltage of ±7 V was obtained for TaAlO CTM device, and it could keep about 60% of initially trapped charges after 10 years. It was suggested that the PBCB difference between high-k composite and p-Si dominates their charge-trapping behaviors.

Why it matters

OpenAlex reports 3 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

The charge-trapping memory (CTM) structures Pt/Al2O3/TaAlO/Al2O3/p-Si and Pt/Al2O3/ZrAlO/Al2O3/p-Si were fabricated by using rf-sputtering and atomic layer deposition techniques, in which the potentials at the bottom of the conduction band (PBCB) of high-k composites TaAlO and ZrAlO were specially designed. With a lower PBCB difference between TaAlO and p-Si than that between ZrAlO and p-Si, TaAlO CTM device shows a better charge-trapping performance. A density of trapped charges 2.88 × 1013/cm2 at an applied voltage of ±7 V was obtained for TaAlO CTM device, and it could keep about 60% of initially trapped charges after 10 years. It was suggested that the PBCB difference between high-k composite and p-Si dominates their charge-trapping behaviors.

Key concepts: Trapping, Conduction band, Charge (physics), Materials science, Composite number, Deposition (geology), Atomic layer deposition, Sputtering

Related papers

Back to paper searchBrowse research topicsOriginal source
Comparative study on the charge-trapping properties of TaAlO and ZrAlO high-k composites with designed band alignment — Research Paper | ScholarLens