1995Applied Physics LettersRequires access

Formation of self-aligned holes in an arbitrary pattern in silicon substrate

Hi‐Deok Lee, Joo‐Ho Lee, Choong‐Ki Kim, Chul‐Hi Han

Open publisher page 8 citations

Abstract

A self-aligning etch method for silicon substrates is presented. A hole pattern is defined on the front side of the silicon substrate while etching of the hole takes place from the back side through the application of a current from the front side of the silicon substrate to a cathode electrode in a solution of HF, HNO3, and H2O. As the etching proceeds, the etched pattern in the back side gradually becomes self-aligned with the front side pattern of the silicon substrate. Twenty five circular holes arranged in a 5×5 array are formed in a boron-doped (100) silicon substrate. The etch method provides control over hole dimensions which are 520 μm in diameter and spaced 520 μm apart. The self-aligning property of the etch method enables the formation of different shaped holes.

About this research paper

What this paper is about

A self-aligning etch method for silicon substrates is presented. A hole pattern is defined on the front side of the silicon substrate while etching of the hole takes place from the back side through the application of a current from the front side of the silicon substrate to a cathode electrode in a solution of HF, HNO3, and H2O. As the etching proceeds, the etched pattern in the back side gradually becomes self-aligned with the front side pattern of the silicon substrate. Twenty five circular holes arranged in a 5×5 array are formed in a boron-doped (100) silicon substrate. The etch method provides control over hole dimensions which are 520 μm in diameter and spaced 520 μm apart. The self-aligning property of the etch method enables the formation of different shaped holes.

Why it matters

OpenAlex reports 8 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

A self-aligning etch method for silicon substrates is presented. A hole pattern is defined on the front side of the silicon substrate while etching of the hole takes place from the back side through the application of a current from the front side of the silicon substrate to a cathode electrode in a solution of HF, HNO3, and H2O. As the etching proceeds, the etched pattern in the back side gradually becomes self-aligned with the front side pattern of the silicon substrate. Twenty five circular holes arranged in a 5×5 array are formed in a boron-doped (100) silicon substrate. The etch method provides control over hole dimensions which are 520 μm in diameter and spaced 520 μm apart. The self-aligning property of the etch method enables the formation of different shaped holes.

Key concepts: Silicon, Substrate (aquarium), Etching (microfabrication), Materials science, Optoelectronics, Boron, Cathode, Doping

Related papers

Back to paper searchBrowse research topicsOriginal source
Formation of self-aligned holes in an arbitrary pattern in silicon substrate — Research Paper | ScholarLens