Spark Plasma Sintering of α-Si3N4 Ceramics with MgO-Al2O3 as Sintering Additives

F. Yan, Fei Chen, Qiang Shen, Lian Meng Zhang

Open full text 11 citations

Abstract

In the present study, α-Si3N4 is prepared by using MgO and Al2O3 as the sintering additives and spark plasma sintering (SPS) technique. The SPS sintering mechanism is discussed. The relationship between the content of sintering additives, sintering temperature and relative densities of the samples is analyzed. The results suggest that when the sintering temperature is 1300-1500°C, the content of sintering additives is 6wt.%-10wt.%, the relative density of sintered samples is 64%-96%. When the sintering temperature reaches 1400°C, the content of sintering additives is 10%, the samples can be fully dense sintered and the relative density can be up to 95%. The sintering mechanism is liquid phase sintering. The bending strength of the sintered samples is 50-403MPa and has a close correlation with the relative density.

About this research paper

What this paper is about

In the present study, α-Si3N4 is prepared by using MgO and Al2O3 as the sintering additives and spark plasma sintering (SPS) technique. The SPS sintering mechanism is discussed. The relationship between the content of sintering additives, sintering temperature and relative densities of the samples is analyzed. The results suggest that when the sintering temperature is 1300-1500°C, the content of sintering additives is 6wt.%-10wt.%, the relative density of sintered samples is 64%-96%. When the sintering temperature reaches 1400°C, the content of sintering additives is 10%, the samples can be fully dense sintered and the relative density can be up to 95%. The sintering mechanism is liquid phase sintering. The bending strength of the sintered samples is 50-403MPa and has a close correlation with the relative density.

Why it matters

OpenAlex reports 11 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

In the present study, α-Si3N4 is prepared by using MgO and Al2O3 as the sintering additives and spark plasma sintering (SPS) technique. The SPS sintering mechanism is discussed. The relationship between the content of sintering additives, sintering temperature and relative densities of the samples is analyzed. The results suggest that when the sintering temperature is 1300-1500°C, the content of sintering additives is 6wt.%-10wt.%, the relative density of sintered samples is 64%-96%. When the sintering temperature reaches 1400°C, the content of sintering additives is 10%, the samples can be fully dense sintered and the relative density can be up to 95%. The sintering mechanism is liquid phase sintering. The bending strength of the sintered samples is 50-403MPa and has a close correlation with the relative density.

Key concepts: Sintering, Spark plasma sintering, Materials science, Relative density, Ceramic, Liquid phase, Composite material, Metallurgy

Related papers

Back to paper searchBrowse research topicsOriginal source
Spark Plasma Sintering of α-Si3N4 Ceramics with MgO-Al2O3 as Sintering Additives — Research Paper | ScholarLens