Preparation and characterization of Ti_3AlC_2/Al composites

Kexi Liu

Open publisher page 0 citations

Abstract

The ternary carbide Ti3AlC2ceramic powders with high purity were fabricated by mechanical alloying and heat treatment technology using Ti,Al and C as starting powders. Ti3AlC2/Al composites were prepared by spark plasma sintering,and the effect of sintering temperature on relative density,hardness and friction coefficient of the composites was investigated.The result demonstrates that with the increase of sintering temperature,relative density and hardness of the composite increase,when the sintering temperature is 550 ℃,relative density and hardness of the composite is 97% and 180HV;the friction coefficient of the composite gradually decreases with the sintering temperature increasing,when the sintering temperature is500 ℃,the friction coefficient reaches the minimum value of about 0.186 9,but when the sintering temperature continues to rise,the friction coefficient becomes larger.

About this research paper

What this paper is about

The ternary carbide Ti3AlC2ceramic powders with high purity were fabricated by mechanical alloying and heat treatment technology using Ti,Al and C as starting powders. Ti3AlC2/Al composites were prepared by spark plasma sintering,and the effect of sintering temperature on relative density,hardness and friction coefficient of the composites was investigated.The result demonstrates that with the increase of sintering temperature,relative density and hardness of the composite increase,when the sintering temperature is 550 ℃,relative density and hardness of the composite is 97% and 180HV;the friction coefficient of the composite gradually decreases with the sintering temperature increasing,when the sintering temperature is500 ℃,the friction coefficient reaches the minimum value of about 0.186 9,but when the sintering temperature continues to rise,the friction coefficient becomes larger.

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

The ternary carbide Ti3AlC2ceramic powders with high purity were fabricated by mechanical alloying and heat treatment technology using Ti,Al and C as starting powders. Ti3AlC2/Al composites were prepared by spark plasma sintering,and the effect of sintering temperature on relative density,hardness and friction coefficient of the composites was investigated.The result demonstrates that with the increase of sintering temperature,relative density and hardness of the composite increase,when the sintering temperature is 550 ℃,relative density and hardness of the composite is 97% and 180HV;the friction coefficient of the composite gradually decreases with the sintering temperature increasing,when the sintering temperature is500 ℃,the friction coefficient reaches the minimum value of about 0.186 9,but when the sintering temperature continues to rise,the friction coefficient becomes larger.

Key concepts: Materials science, Spark plasma sintering, Sintering, Relative density, Composite number, Composite material, Ternary operation, Carbide

Related papers

Back to paper searchBrowse research topicsOriginal source
Preparation and characterization of Ti_3AlC_2/Al composites — Research Paper | ScholarLens