2001Science and Technology of Welding & JoiningRequires access

Effect of surface condition and bonding pressure on quality of diffusion bonded high purity copper for linear collider accelerator structures

J. W. Elmer, J. Klingman, K. van Bibber

Open publisher page 12 citations

Abstract

Tests have been carried out to assess the feasibility of diffusion bonding as a fabrication technology for vacuum tight joints in linear accelerator cells for the Next Linear Collider. High purity copper specimens were diffusion bonded over a range of temperatures from 400 to 1000°C, under high (3.45 MPa) and low (3.45 kPa) bonding pressures, and at two different diamond machined surface finishes. Experiments showed that diffusion bonds with strengths equal to, or greater than, that of silver brazed joints could be made at temperatures ≥700°C at the 3.45 MPa bonding pressure, or ≥800°C at the 3.45 kPa bonding pressure. Partial strength diffusion bonds were made at temperatures as low as 400°C at the high bonding pressure, whereas no bonding (zero strength) was observed at temperatures below 700°C at the low bonding pressure. Observations of the fracture surfaces of the diffusion bonded specimens showed that bonding begins by point asperity contact. At low bonding pressures, surfaces created by diamond turning of annealed copper specimens produce higher strength bonds than those created by diamond flycutting of unannealed surfaces, whereas at higher bonding pressures the effect of surface finish was less important.

About this research paper

What this paper is about

Tests have been carried out to assess the feasibility of diffusion bonding as a fabrication technology for vacuum tight joints in linear accelerator cells for the Next Linear Collider. High purity copper specimens were diffusion bonded over a range of temperatures from 400 to 1000°C, under high (3.45 MPa) and low (3.45 kPa) bonding pressures, and at two different diamond machined surface finishes. Experiments showed that diffusion bonds with strengths equal to, or greater than, that of silver brazed joints could be made at temperatures ≥700°C at the 3.45 MPa bonding pressure, or ≥800°C at the 3.45 kPa bonding pressure. Partial strength diffusion bonds were made at temperatures as low as 400°C at the high bonding pressure, whereas no bonding (zero strength) was observed at temperatures below 700°C at the low bonding pressure. Observations of the fracture surfaces of the diffusion bonded specimens showed that bonding begins by point asperity contact. At low bonding pressures, surfaces created by diamond turning of annealed copper specimens produce higher strength bonds than those created by diamond flycutting of unannealed surfaces, whereas at higher bonding pressures the effect of surface finish was less important.

Why it matters

OpenAlex reports 12 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Tests have been carried out to assess the feasibility of diffusion bonding as a fabrication technology for vacuum tight joints in linear accelerator cells for the Next Linear Collider. High purity copper specimens were diffusion bonded over a range of temperatures from 400 to 1000°C, under high (3.45 MPa) and low (3.45 kPa) bonding pressures, and at two different diamond machined surface finishes. Experiments showed that diffusion bonds with strengths equal to, or greater than, that of silver brazed joints could be made at temperatures ≥700°C at the 3.45 MPa bonding pressure, or ≥800°C at the 3.45 kPa bonding pressure. Partial strength diffusion bonds were made at temperatures as low as 400°C at the high bonding pressure, whereas no bonding (zero strength) was observed at temperatures below 700°C at the low bonding pressure. Observations of the fracture surfaces of the diffusion bonded specimens showed that bonding begins by point asperity contact. At low bonding pressures, surfaces created by diamond turning of annealed copper specimens produce higher strength bonds than those created by diamond flycutting of unannealed surfaces, whereas at higher bonding pressures the effect of surface finish was less important.

Key concepts: Diffusion bonding, Materials science, Thermocompression bonding, Anodic bonding, Copper, Composite material, Diamond, Metallurgy

Related papers

Back to paper searchBrowse research topicsOriginal source
Effect of surface condition and bonding pressure on quality of diffusion bonded high purity copper for linear collider accelerator structures — Research Paper | ScholarLens