Effect of Reheating Conditions of Semi-Solid Aluminum Alloy on Globular Microstructure

Seong-Su Gang, Chung-Gil Gang, Yeong-Jin Do

Open publisher page 3 citations

Abstract

A semi-solid forming has a lot of advantages compared to the die casting. squeeze casting and conventional forging. therefore, semi-solid forming process is now becoming industrial interest for the production of metal components and metal matrix composites. However the material behaviour in the semi-solid temperature range is not sufficiently known although it controls the whole process through forces and geometry evolutions because the behaviour of metal slurries is complex. The semi-solid materials(SSMs) fabricated under electric-magnetic stirring condition is necessary to be applicated in forming process. A reheating conditions were studied with the reheating time holding time and reheating temperatures. The microstructure of SSM(specimen size : d39h85) at the condition of heating time 10min and heating temperature 590 is the most globular and finest one. The microstructure of SSM(specimen size : d76h60) reheated under the three step reheating conditions is most globular and finest.

About this research paper

What this paper is about

A semi-solid forming has a lot of advantages compared to the die casting. squeeze casting and conventional forging. therefore, semi-solid forming process is now becoming industrial interest for the production of metal components and metal matrix composites. However the material behaviour in the semi-solid temperature range is not sufficiently known although it controls the whole process through forces and geometry evolutions because the behaviour of metal slurries is complex. The semi-solid materials(SSMs) fabricated under electric-magnetic stirring condition is necessary to be applicated in forming process. A reheating conditions were studied with the reheating time holding time and reheating temperatures. The microstructure of SSM(specimen size : d39h85) at the condition of heating time 10min and heating temperature 590 is the most globular and finest one. The microstructure of SSM(specimen size : d76h60) reheated under the three step reheating conditions is most globular and finest.

Why it matters

OpenAlex reports 3 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

A semi-solid forming has a lot of advantages compared to the die casting. squeeze casting and conventional forging. therefore, semi-solid forming process is now becoming industrial interest for the production of metal components and metal matrix composites. However the material behaviour in the semi-solid temperature range is not sufficiently known although it controls the whole process through forces and geometry evolutions because the behaviour of metal slurries is complex. The semi-solid materials(SSMs) fabricated under electric-magnetic stirring condition is necessary to be applicated in forming process. A reheating conditions were studied with the reheating time holding time and reheating temperatures. The microstructure of SSM(specimen size : d39h85) at the condition of heating time 10min and heating temperature 590 is the most globular and finest one. The microstructure of SSM(specimen size : d76h60) reheated under the three step reheating conditions is most globular and finest.

Key concepts: Microstructure, Materials science, Forging, Alloy, Casting, Metallurgy, Slurry, Aluminium