Use of pea coke in a blast furnace with a volume of 3,200 m[sup 3] as a partial replacement for blast furnace coke

T. Misiun, Wladyslaw Woźniacki, J Wyroslak

Open publisher page 0 citations

Abstract

Evaluates effects of partial replacement of standard blast furnace coke with pea coke with a grain size from 10 to 245 mm on operation of a blast furnace and on coke consumption rates. Coke abrasion was investigated under laboratory conditions at 1,000 C. Reactivity of pea coke and that of standard blast furnace coke was comparatively evaluated at 900 C, 1,000 C and 1,100 C. Effects of partial replacement of standard blast furnace coke with pea coke were investigated under operating condition in a blast furnace with a volume of 3,200 m[sup 3]. Investigations showed that replacing 8-9% blast furnace coke with pea coke did not negatively influence the permeability of a blast-furnace charge. Pea coke should be characterized by reactivity higher than that of standard blast furnace coke. 3 refs.

About this research paper

What this paper is about

Evaluates effects of partial replacement of standard blast furnace coke with pea coke with a grain size from 10 to 245 mm on operation of a blast furnace and on coke consumption rates. Coke abrasion was investigated under laboratory conditions at 1,000 C. Reactivity of pea coke and that of standard blast furnace coke was comparatively evaluated at 900 C, 1,000 C and 1,100 C. Effects of partial replacement of standard blast furnace coke with pea coke were investigated under operating condition in a blast furnace with a volume of 3,200 m[sup 3]. Investigations showed that replacing 8-9% blast furnace coke with pea coke did not negatively influence the permeability of a blast-furnace charge. Pea coke should be characterized by reactivity higher than that of standard blast furnace coke. 3 refs.

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Evaluates effects of partial replacement of standard blast furnace coke with pea coke with a grain size from 10 to 245 mm on operation of a blast furnace and on coke consumption rates. Coke abrasion was investigated under laboratory conditions at 1,000 C. Reactivity of pea coke and that of standard blast furnace coke was comparatively evaluated at 900 C, 1,000 C and 1,100 C. Effects of partial replacement of standard blast furnace coke with pea coke were investigated under operating condition in a blast furnace with a volume of 3,200 m[sup 3]. Investigations showed that replacing 8-9% blast furnace coke with pea coke did not negatively influence the permeability of a blast-furnace charge. Pea coke should be characterized by reactivity higher than that of standard blast furnace coke. 3 refs.

Key concepts: Blast furnace, Coke, Coke strength after reaction, Metallurgy, Blast furnace gas, Petroleum coke, Materials science, Chemistry

Related papers

Back to paper searchBrowse research topicsOriginal source
Use of pea coke in a blast furnace with a volume of 3,200 m[sup 3] as a partial replacement for blast furnace coke — Research Paper | ScholarLens