The Effect of Hydrothermal Synthesis Parameters on the Formation of Sodium Bismuth Titanate
Elena A. Reshetnikova, Inna V. Lisnevskaya, Ekaterina A. Zalyubovskaya, Vera V. Butova, Alexander V. Soldatov
Abstract
Open-access reader
Elena A. Reshetnikova, Inna V. Lisnevskaya, Ekaterina A. Zalyubovskaya, Vera V. Butova, Alexander V. Soldatov
Abstract
Open-access reader
We report the effect of various Bi:Ti ratios x:1 (x = 0.5–3) on the phase formation of sodium-bismuth titanate Na0.5Bi0.5TiO3 (NBT) during hydrothermal synthesis (230°С, 3 MPa, 96 h) from titanium oxide and bismuth hydroxide in 20 M NaOH solution. It was shown that single-phase ceramics with perovskite structure could be obtained at x = 0.5–0.9 using the hot-pressing technique (1025°С, 60 MPa, 1 h). At x = 1, hydrothermal synthesis results in single-phase samples, while, after sintering, the admixture of Na2Ti3O7 was detected. At x = 2 and 3, samples contained admixtures after hydrothermal synthesis. The x–value does not significantly affect the composition of perovskite-like products despite the excess of bismuth in the system. The chemical composition of the samples with x = 0.5–0.9 corresponds to the general formula Na0.60–0.69Bi0.40–0.31TiO2.9–2.81δ0.10–0.19 (where δ represents vacancies in oxygen sublattice). The Bi3+ content in the samples is underestimated due to the solubility of its hydroxide in a 20 M alkali solution. The properties of ceramics are not significantly affected by x values, and materials exhibit following average characteristics: electrical resistivity 1.3 × 109 Ohm∙cm, tanδ = 0.15, Кр = 0.1, d31 = 6.7 and d33 = 9.5 pC/N, g31 = 2.34 and g33 = 3 mV∙m/N.
OpenAlex reports 8 citations for this work. Citation counts describe recorded attention and do not establish research quality.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
We report the effect of various Bi:Ti ratios x:1 (x = 0.5–3) on the phase formation of sodium-bismuth titanate Na0.5Bi0.5TiO3 (NBT) during hydrothermal synthesis (230°С, 3 MPa, 96 h) from titanium oxide and bismuth hydroxide in 20 M NaOH solution. It was shown that single-phase ceramics with perovskite structure could be obtained at x = 0.5–0.9 using the hot-pressing technique (1025°С, 60 MPa, 1 h). At x = 1, hydrothermal synthesis results in single-phase samples, while, after sintering, the admixture of Na2Ti3O7 was detected. At x = 2 and 3, samples contained admixtures after hydrothermal synthesis. The x–value does not significantly affect the composition of perovskite-like products despite the excess of bismuth in the system. The chemical composition of the samples with x = 0.5–0.9 corresponds to the general formula Na0.60–0.69Bi0.40–0.31TiO2.9–2.81δ0.10–0.19 (where δ represents vacancies in oxygen sublattice). The Bi3+ content in the samples is underestimated due to the solubility of its hydroxide in a 20 M alkali solution. The properties of ceramics are not significantly affected by x values, and materials exhibit following average characteristics: electrical resistivity 1.3 × 109 Ohm∙cm, tanδ = 0.15, Кр = 0.1, d31 = 6.7 and d33 = 9.5 pC/N, g31 = 2.34 and g33 = 3 mV∙m/N.
Key concepts: Chemistry, Bismuth, Hydrothermal circulation, Bismuth titanate, Sodium hydroxide, Perovskite (structure), Hydrothermal synthesis, Sintering