Effect of the sintering temperature on microstructure and properties of Al 2 O 3 –Cu–Ni hybrid composites obtained by PPS
Justyna Zygmuntowicz, Paweł Falkowski, Marcin Wachowski, Konrad Cymerman, Paulina Piotrkiewicz, Waldemar Kaszuwara
Abstract
Justyna Zygmuntowicz, Paweł Falkowski, Marcin Wachowski, Konrad Cymerman, Paulina Piotrkiewicz, Waldemar Kaszuwara
Abstract
Abstract In the present research, the influence of sintering temperature on the microstructure and properties of Al 2 O 3 –Cu–Ni hybrid composites prepared by the Pulse Plasma Sintering (PPS) technique were described. In this research, three temperatures have been selected: 1250°C, 1300°C, and 1350°C. SEM observations were carried out to determine the distribution of the metallic phase in the composite depending on the sintering temperature. The conducted experiments and microscopic observations enabled a better understanding of the phenomena occurring between the ceramic matrix and metallic phase in the obtained materials. The mechanical properties like a hardness and fracture toughness were measured. The technology applied allowed us to obtain ceramic‐metal composites with a homogeneous microstructure. It was found that the sintering temperature influences the selected physical and mechanical properties of the composites produced. It was found that samples produced at 1300°C are characterized by the highest relative density and the mechanical properties.
OpenAlex reports 12 citations for this work. Citation counts describe recorded attention and do not establish research quality.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
Abstract In the present research, the influence of sintering temperature on the microstructure and properties of Al 2 O 3 –Cu–Ni hybrid composites prepared by the Pulse Plasma Sintering (PPS) technique were described. In this research, three temperatures have been selected: 1250°C, 1300°C, and 1350°C. SEM observations were carried out to determine the distribution of the metallic phase in the composite depending on the sintering temperature. The conducted experiments and microscopic observations enabled a better understanding of the phenomena occurring between the ceramic matrix and metallic phase in the obtained materials. The mechanical properties like a hardness and fracture toughness were measured. The technology applied allowed us to obtain ceramic‐metal composites with a homogeneous microstructure. It was found that the sintering temperature influences the selected physical and mechanical properties of the composites produced. It was found that samples produced at 1300°C are characterized by the highest relative density and the mechanical properties.
Key concepts: Materials science, Microstructure, Sintering, Composite material, Ceramic, Relative density, Fracture toughness, Composite number