Mohamed M. Awad, Lamees Albedaiwi, Ahmed Almahdy, Rawaiz Khan, Nick Silikas, Muhanad M. Hatamleh, Fahad Alkhtani, Ali Alrahlah

Open full text 31 citations

Abstract

BACKGROUND: The aim of this study was to evaluate the effect of universal adhesives (UA) and silane on the microtensile bond strength (μTBS) of resin cement to a hybrid ceramic Vita Enamic (VE). METHODS: VE specimens were acid etched using hydrofluoric acid (HF) and were assigned to three groups (n = 10) based on the applied bonding technique. In group 1 (S), a silane-based primer was used as a surface treatment prior to the application of a resin cement (Variolink Esthetic DC). In group 2, a silane-containing UA, Clearfil Universal Bond (CUB) was used for the surface treatment, and in group 3, A silane-free UA, Tetric N-Bond Universal (TNU) was used for surface treatment. Resin cement build-ups were prepared. The bonded specimens were sectioned into resin-ceramic beams. Half of the beams of each group were stored for 24 h at 37 °C and the other half were subjected to a thermo-cycling aging. The microtensile bond strength (μTBS) was measured at a crosshead speed of 0.5 mm/min. Failure modes were assessed accordingly. Data were analyzed using a) two-way analysis of variance ANOVA followed by one-way ANOVA and Tukey tests between groups and b) independent t-test to detect differences (α = 0.05) for each group. The surface topographies of the ceramic surface were evaluated using scanning electron microscopy. RESULTS: The results showed that silane-based primer (S) application resulted in significantly higher (p < 0.05) μTBS values after 24 h and after thermocycling compared to both silane-containing UA (CUB) and silane-free UA (TNU). The μTBS values of all groups were significantly reduced after thermocycling. No statistically significant difference was observed between the μTBS of CUB and TNU after 24 h. However, TNU showed significantly higher μTBS after thermocycling. Different failure modes were observed, and adhesive failure was the most common in all groups. Marked surface topographic changes were observed following HF etching. CONCLUSION: It is concluded that, the UAs tested cannot be recommended as substitutes to the silanization of Hybrid ceramic.

Open-access reader

About this research paper

What this paper is about

BACKGROUND: The aim of this study was to evaluate the effect of universal adhesives (UA) and silane on the microtensile bond strength (μTBS) of resin cement to a hybrid ceramic Vita Enamic (VE). METHODS: VE specimens were acid etched using hydrofluoric acid (HF) and were assigned to three groups (n = 10) based on the applied bonding technique. In group 1 (S), a silane-based primer was used as a surface treatment prior to the application of a resin cement (Variolink Esthetic DC). In group 2, a silane-containing UA, Clearfil Universal Bond (CUB) was used for the surface treatment, and in group 3, A silane-free UA, Tetric N-Bond Universal (TNU) was used for surface treatment. Resin cement build-ups were prepared. The bonded specimens were sectioned into resin-ceramic beams. Half of the beams of each group were stored for 24 h at 37 °C and the other half were subjected to a thermo-cycling aging. The microtensile bond strength (μTBS) was measured at a crosshead speed of 0.5 mm/min. Failure modes were assessed accordingly. Data were analyzed using a) two-way analysis of variance ANOVA followed by one-way ANOVA and Tukey tests between groups and b) independent t-test to detect differences (α = 0.05) for each group. The surface topographies of the ceramic surface were evaluated using scanning electron microscopy. RESULTS: The results showed that silane-based primer (S) application resulted in significantly higher (p < 0.05) μTBS values after 24 h and after thermocycling compared to both silane-containing UA (CUB) and silane-free UA (TNU). The μTBS values of all groups were significantly reduced after thermocycling. No statistically significant difference was observed between the μTBS of CUB and TNU after 24 h. However, TNU showed significantly higher μTBS after thermocycling. Different failure modes were observed, and adhesive failure was the most common in all groups. Marked surface topographic changes were observed following HF etching. CONCLUSION: It is concluded that, the UAs tested cannot be recommended as substitutes to the silanization of Hybrid ceramic.

Why it matters

OpenAlex reports 31 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

BACKGROUND: The aim of this study was to evaluate the effect of universal adhesives (UA) and silane on the microtensile bond strength (μTBS) of resin cement to a hybrid ceramic Vita Enamic (VE). METHODS: VE specimens were acid etched using hydrofluoric acid (HF) and were assigned to three groups (n = 10) based on the applied bonding technique. In group 1 (S), a silane-based primer was used as a surface treatment prior to the application of a resin cement (Variolink Esthetic DC). In group 2, a silane-containing UA, Clearfil Universal Bond (CUB) was used for the surface treatment, and in group 3, A silane-free UA, Tetric N-Bond Universal (TNU) was used for surface treatment. Resin cement build-ups were prepared. The bonded specimens were sectioned into resin-ceramic beams. Half of the beams of each group were stored for 24 h at 37 °C and the other half were subjected to a thermo-cycling aging. The microtensile bond strength (μTBS) was measured at a crosshead speed of 0.5 mm/min. Failure modes were assessed accordingly. Data were analyzed using a) two-way analysis of variance ANOVA followed by one-way ANOVA and Tukey tests between groups and b) independent t-test to detect differences (α = 0.05) for each group. The surface topographies of the ceramic surface were evaluated using scanning electron microscopy. RESULTS: The results showed that silane-based primer (S) application resulted in significantly higher (p < 0.05) μTBS values after 24 h and after thermocycling compared to both silane-containing UA (CUB) and silane-free UA (TNU). The μTBS values of all groups were significantly reduced after thermocycling. No statistically significant difference was observed between the μTBS of CUB and TNU after 24 h. However, TNU showed significantly higher μTBS after thermocycling. Different failure modes were observed, and adhesive failure was the most common in all groups. Marked surface topographic changes were observed following HF etching. CONCLUSION: It is concluded that, the UAs tested cannot be recommended as substitutes to the silanization of Hybrid ceramic.

Key concepts: Silane, Bond strength, Adhesive, Universal testing machine, Materials science, Ceramic, Composite material, Cement

Related papers

Back to paper searchBrowse research topicsOriginal source
Effect of universal adhesives on microtensile bond strength to hybrid ceramic — Research Paper | ScholarLens