Growth of Cubic GaN by MOCVD at High Temperature
Fu Yi, Sun Yuanping, Shen Xiaoming, Shunfeng Li, Feng Zhihong, Lihong Duan, Hai Wang, Yang Hui
Abstract
Fu Yi, Sun Yuanping, Shen Xiaoming, Shunfeng Li, Feng Zhihong, Lihong Duan, Hai Wang, Yang Hui
Abstract
High quality cubic GaN (c-GaN) is grown by metalorganic vapor deposition (MOCVD) at an increased growth temperature of 900 ℃, with the growth rate of 1.6 μm/h. The full width at half maximum (FWHM) of room temperature photoluminescence (PL) for the high temperature grown GaN film is 48meV. It is smaller than that of the sample grown at 830 ℃. In X-ray diffraction (XRD) measurement, the high temperature grown GaN shows a (002) peak at 20° with a FWHM of 21'. It can be concluded that, although c-GaN is of metastable phase, high growth temperature is still beneficial to the improvement in its crystal quality. The relationship between the growth rate and growth temperature is also discussed.
A significance statement is not available in the OpenAlex record.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
High quality cubic GaN (c-GaN) is grown by metalorganic vapor deposition (MOCVD) at an increased growth temperature of 900 ℃, with the growth rate of 1.6 μm/h. The full width at half maximum (FWHM) of room temperature photoluminescence (PL) for the high temperature grown GaN film is 48meV. It is smaller than that of the sample grown at 830 ℃. In X-ray diffraction (XRD) measurement, the high temperature grown GaN shows a (002) peak at 20° with a FWHM of 21'. It can be concluded that, although c-GaN is of metastable phase, high growth temperature is still beneficial to the improvement in its crystal quality. The relationship between the growth rate and growth temperature is also discussed.
Key concepts: Metalorganic vapour phase epitaxy, Full width at half maximum, Materials science, Photoluminescence, Growth rate, Chemical vapor deposition, Metastability, Diffraction