Activating-tungsten inert-gas welding for TA15 titanium alloy

Dong Zhan-gui

Open publisher page 0 citations

Abstract

In the view of weld form,weld pore,joint mechanical properties,microstructur and joint anti-erode performance,etc, A-TIG(activating-tungsten inert-gas) welding for TA15 titanium alloy has been studied.The experimental results show that compared with conventional TIG(tungsten inert-gas) welding,A-TIG welding can increase weld bead penetration while decrease weld bead width,and can decrease the number of pore effectively,also can enhance joint tensile property and bend property.Heat-affected zone of A-TIG welding is narrower, and its microstructure is finer in comparison with TIG welding,while their microstructures of weld zone are almost same.The activating flux doesn't affect joint anti-erode performance.A-TIG welding is superior to conventional TIG welding for TA15 titanium alloy.

About this research paper

What this paper is about

In the view of weld form,weld pore,joint mechanical properties,microstructur and joint anti-erode performance,etc, A-TIG(activating-tungsten inert-gas) welding for TA15 titanium alloy has been studied.The experimental results show that compared with conventional TIG(tungsten inert-gas) welding,A-TIG welding can increase weld bead penetration while decrease weld bead width,and can decrease the number of pore effectively,also can enhance joint tensile property and bend property.Heat-affected zone of A-TIG welding is narrower, and its microstructure is finer in comparison with TIG welding,while their microstructures of weld zone are almost same.The activating flux doesn't affect joint anti-erode performance.A-TIG welding is superior to conventional TIG welding for TA15 titanium alloy.

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

In the view of weld form,weld pore,joint mechanical properties,microstructur and joint anti-erode performance,etc, A-TIG(activating-tungsten inert-gas) welding for TA15 titanium alloy has been studied.The experimental results show that compared with conventional TIG(tungsten inert-gas) welding,A-TIG welding can increase weld bead penetration while decrease weld bead width,and can decrease the number of pore effectively,also can enhance joint tensile property and bend property.Heat-affected zone of A-TIG welding is narrower, and its microstructure is finer in comparison with TIG welding,while their microstructures of weld zone are almost same.The activating flux doesn't affect joint anti-erode performance.A-TIG welding is superior to conventional TIG welding for TA15 titanium alloy.

Key concepts: Welding, Gas tungsten arc welding, Materials science, Inert gas, Heat-affected zone, Metallurgy, Tungsten, Welding joint

Related papers

Back to paper searchBrowse research topicsOriginal source
Activating-tungsten inert-gas welding for TA15 titanium alloy — Research Paper | ScholarLens