New Process to Recover Coarse Ilmenite in Midi Titanium Concentration Plant of Panzhihua
Meng Chang-chun
Abstract
Meng Chang-chun
Abstract
After analyzing the main problems in the existing production line for reclaiming coarse ilmenite in Midi Titanium Concentration Plant of Panzhihua,a new process was proposed,with high-intensity magnetic separation-flotation as the principal approach and with MOH-2 as the collector.The onsite production proves that coarse ilmenite can be effectively recovered with this new technique,and the upper limit of ilmenite feed size for flotation can be increased from 0.1 mm to 0.154 mm.
A significance statement is not available in the OpenAlex record.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
After analyzing the main problems in the existing production line for reclaiming coarse ilmenite in Midi Titanium Concentration Plant of Panzhihua,a new process was proposed,with high-intensity magnetic separation-flotation as the principal approach and with MOH-2 as the collector.The onsite production proves that coarse ilmenite can be effectively recovered with this new technique,and the upper limit of ilmenite feed size for flotation can be increased from 0.1 mm to 0.154 mm.
Key concepts: Ilmenite, Titanium, Metallurgy, Materials science, PUREX, Pulp and paper industry, Environmental science, Extraction (chemistry)