2004•Journal of Sichuan UniversityRequires access

Electrochemical Preparation of Sodium Ferrate(VI) Using Silicon Iron as Anode in Non-Diaphragm Electrobath

Yongchun Liu, Jiali Xie

Open publisher page 1 citations

Abstract

Using silicon iron as anode to preparation sodium ferrate(Ⅵ) in non-diaphragm electrobath.The maximum current yield was reached to 43.0%(concentration of ferrate(Ⅵ) is( 0.079mol·L~(-1) )) under condition that take 40% sodium hydrate as electrolyte in which containing 1% sodium silicate,reaction temperature is around 35℃,current density equals 40mA·cm~(-2) and electrolysis duration is 180mins.It proved that silicon iron anode is better than other reported anode,such as carbon iron or zinc white iron anode ect..

About this research paper

What this paper is about

Using silicon iron as anode to preparation sodium ferrate(Ⅵ) in non-diaphragm electrobath.The maximum current yield was reached to 43.0%(concentration of ferrate(Ⅵ) is( 0.079mol·L~(-1) )) under condition that take 40% sodium hydrate as electrolyte in which containing 1% sodium silicate,reaction temperature is around 35℃,current density equals 40mA·cm~(-2) and electrolysis duration is 180mins.It proved that silicon iron anode is better than other reported anode,such as carbon iron or zinc white iron anode ect..

Why it matters

OpenAlex reports 1 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Using silicon iron as anode to preparation sodium ferrate(Ⅵ) in non-diaphragm electrobath.The maximum current yield was reached to 43.0%(concentration of ferrate(Ⅵ) is( 0.079mol·L~(-1) )) under condition that take 40% sodium hydrate as electrolyte in which containing 1% sodium silicate,reaction temperature is around 35℃,current density equals 40mA·cm~(-2) and electrolysis duration is 180mins.It proved that silicon iron anode is better than other reported anode,such as carbon iron or zinc white iron anode ect..

Key concepts: Anode, Electrolysis, Silicon, Electrolyte, Electrochemistry, Sodium silicate, Sodium, Inorganic chemistry