2013•Physical Testing and Chemical AnalysisRequires access

HG-ICP-AES Determination of As,Sb and Bi in Ductile Iron

YE Jian-pin

Open publisher page 0 citations

Abstract

HG-ICP-AES was applied to the determination of As,Sb and Bi in ductile iron.The sample was dissolved in HCl(1+1)solution and H_2O_2.Hydrides of As,Sb and Bi were generated by reacting with 10g·L~(-1) KBH_4 solution(dissolved in 4g·L~(-1)NaOH solution).Analytical spectral lines of 193.696,206.838 and 223.061 nm were chosen for the determination of As,Sb and Bi respectively.Linear relationships between values of emission intensity and mass concentration of As,Sb and Bi were kept in the same range within 1.6mg·L~(-1),with their detection limits(3S/N)of 0.39,0.37 and 0.77μg·L~(-1)respectively.The proposed method was applied to the analysis of 4 standard samples of ductile iron,giving results in consistency with the certified values.Values of recovery obtained by standard addition method were found in the range of 94.0%-105%with RSD's(n=6)in the range of 0.34%-2.6%.

About this research paper

What this paper is about

HG-ICP-AES was applied to the determination of As,Sb and Bi in ductile iron.The sample was dissolved in HCl(1+1)solution and H_2O_2.Hydrides of As,Sb and Bi were generated by reacting with 10g·L~(-1) KBH_4 solution(dissolved in 4g·L~(-1)NaOH solution).Analytical spectral lines of 193.696,206.838 and 223.061 nm were chosen for the determination of As,Sb and Bi respectively.Linear relationships between values of emission intensity and mass concentration of As,Sb and Bi were kept in the same range within 1.6mg·L~(-1),with their detection limits(3S/N)of 0.39,0.37 and 0.77μg·L~(-1)respectively.The proposed method was applied to the analysis of 4 standard samples of ductile iron,giving results in consistency with the certified values.Values of recovery obtained by standard addition method were found in the range of 94.0%-105%with RSD's(n=6)in the range of 0.34%-2.6%.

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

HG-ICP-AES was applied to the determination of As,Sb and Bi in ductile iron.The sample was dissolved in HCl(1+1)solution and H_2O_2.Hydrides of As,Sb and Bi were generated by reacting with 10g·L~(-1) KBH_4 solution(dissolved in 4g·L~(-1)NaOH solution).Analytical spectral lines of 193.696,206.838 and 223.061 nm were chosen for the determination of As,Sb and Bi respectively.Linear relationships between values of emission intensity and mass concentration of As,Sb and Bi were kept in the same range within 1.6mg·L~(-1),with their detection limits(3S/N)of 0.39,0.37 and 0.77μg·L~(-1)respectively.The proposed method was applied to the analysis of 4 standard samples of ductile iron,giving results in consistency with the certified values.Values of recovery obtained by standard addition method were found in the range of 94.0%-105%with RSD's(n=6)in the range of 0.34%-2.6%.

Key concepts: Analytical Chemistry (journal), Inductively coupled plasma atomic emission spectroscopy, Standard addition, Standard solution, Certified reference materials, Detection limit, Materials science, Chemistry

Related papers

Back to paper searchBrowse research topicsOriginal source
HG-ICP-AES Determination of As,Sb and Bi in Ductile Iron — Research Paper | ScholarLens