Microstructure and properties of aluminum brass with Ce

Dezhi Zhang

Open publisher page 1 citations

Abstract

The processing abilities,structures and corrosion properties of the ceric aluminum brass and the arsenical aluminum brass were studied by means of metallographic analysis,microhardness measurement,mass loss measurement,electrochemical testing and scanning electron microscopy.The results show that the suitable hot-rolling temperature of the alloy with Ce is between 700 and 750 ℃;it has excellent cold-working capability,and the annealed structure is fine and homogeneous after annealing at 700 ℃ for 1 h;the recrystallization grains are about 50 μm.In the process of corrosion in 3.5% NaCl solution,the ceric aluminum brass forms a homogeneous and tight corrosion film on the surface,which can inhibit the diffusion of Zn from the surface of matrix to the solution,and restrain the dezincification to a certain degree.The corrosion resistance of the ceric aluminum brass is slightly better than that of the arsenical aluminum brass,the corrosion rate is 6.2×10?3 mm/a.

About this research paper

What this paper is about

The processing abilities,structures and corrosion properties of the ceric aluminum brass and the arsenical aluminum brass were studied by means of metallographic analysis,microhardness measurement,mass loss measurement,electrochemical testing and scanning electron microscopy.The results show that the suitable hot-rolling temperature of the alloy with Ce is between 700 and 750 ℃;it has excellent cold-working capability,and the annealed structure is fine and homogeneous after annealing at 700 ℃ for 1 h;the recrystallization grains are about 50 μm.In the process of corrosion in 3.5% NaCl solution,the ceric aluminum brass forms a homogeneous and tight corrosion film on the surface,which can inhibit the diffusion of Zn from the surface of matrix to the solution,and restrain the dezincification to a certain degree.The corrosion resistance of the ceric aluminum brass is slightly better than that of the arsenical aluminum brass,the corrosion rate is 6.2×10?3 mm/a.

Why it matters

OpenAlex reports 1 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

The processing abilities,structures and corrosion properties of the ceric aluminum brass and the arsenical aluminum brass were studied by means of metallographic analysis,microhardness measurement,mass loss measurement,electrochemical testing and scanning electron microscopy.The results show that the suitable hot-rolling temperature of the alloy with Ce is between 700 and 750 ℃;it has excellent cold-working capability,and the annealed structure is fine and homogeneous after annealing at 700 ℃ for 1 h;the recrystallization grains are about 50 μm.In the process of corrosion in 3.5% NaCl solution,the ceric aluminum brass forms a homogeneous and tight corrosion film on the surface,which can inhibit the diffusion of Zn from the surface of matrix to the solution,and restrain the dezincification to a certain degree.The corrosion resistance of the ceric aluminum brass is slightly better than that of the arsenical aluminum brass,the corrosion rate is 6.2×10?3 mm/a.

Key concepts: Brass, Materials science, Corrosion, Metallurgy, Aluminium, Microstructure, Annealing (glass), Alloy

Related papers

Back to paper searchBrowse research topicsOriginal source
Microstructure and properties of aluminum brass with Ce — Research Paper | ScholarLens