Abstract

With the feature of finely-dissemination particle and complex mineral composition,oolitic hematite is considered to be the ore dressing difficult problem in the world.beneficiation process research on refractory oolitic hematite in Zhangjiakou Area are introduced according ore properties.Both using high intensity magnetic separation-reverse flotation flowsheet or using high intensity magnetic separation-gravity separation flowsheet,obtaining iron concentrates grading 62% Fe at the recovery of less than 50% each.So roasting-low intensity magnetic separation is adopted.with roasting temperature of 850℃,time for 75~90min and ore-coal ratio of 11,the grinding fineness of-0.076mm 80%,magnetic intensity of 80KA/m,gaining the iron concentrates assaying 63.06% Fe at the recovery of 86.05%.

About this research paper

What this paper is about

With the feature of finely-dissemination particle and complex mineral composition,oolitic hematite is considered to be the ore dressing difficult problem in the world.beneficiation process research on refractory oolitic hematite in Zhangjiakou Area are introduced according ore properties.Both using high intensity magnetic separation-reverse flotation flowsheet or using high intensity magnetic separation-gravity separation flowsheet,obtaining iron concentrates grading 62% Fe at the recovery of less than 50% each.So roasting-low intensity magnetic separation is adopted.with roasting temperature of 850℃,time for 75~90min and ore-coal ratio of 11,the grinding fineness of-0.076mm 80%,magnetic intensity of 80KA/m,gaining the iron concentrates assaying 63.06% Fe at the recovery of 86.05%.

Why it matters

OpenAlex reports 4 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

With the feature of finely-dissemination particle and complex mineral composition,oolitic hematite is considered to be the ore dressing difficult problem in the world.beneficiation process research on refractory oolitic hematite in Zhangjiakou Area are introduced according ore properties.Both using high intensity magnetic separation-reverse flotation flowsheet or using high intensity magnetic separation-gravity separation flowsheet,obtaining iron concentrates grading 62% Fe at the recovery of less than 50% each.So roasting-low intensity magnetic separation is adopted.with roasting temperature of 850℃,time for 75~90min and ore-coal ratio of 11,the grinding fineness of-0.076mm 80%,magnetic intensity of 80KA/m,gaining the iron concentrates assaying 63.06% Fe at the recovery of 86.05%.

Key concepts: Hematite, Beneficiation, Roasting, Magnetic separation, Fineness, Grinding, Metallurgy, Iron ore