Study on Copper Recovery of Lead-zinc Smelting Waste
Yong Liu
Abstract
Yong Liu
Abstract
According to problems of superfine dissemination size and low liberation degree of lead and zinc smelting waste in one company,the way of two stage rougher flotation and one stage scavenging,two segment regrinding and two cleaning operations of rough concentrate is used under the condition of grinding fineness of 85%-0.074 mm.Through the process above,the grinding fineness is 90%-0.049 mm,and a copper concentrate containing 20.36%Cu and 478.87 g/t Ag is obtained,with 64.86% Cu and 59.79% Ag recovered.
A significance statement is not available in the OpenAlex record.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
According to problems of superfine dissemination size and low liberation degree of lead and zinc smelting waste in one company,the way of two stage rougher flotation and one stage scavenging,two segment regrinding and two cleaning operations of rough concentrate is used under the condition of grinding fineness of 85%-0.074 mm.Through the process above,the grinding fineness is 90%-0.049 mm,and a copper concentrate containing 20.36%Cu and 478.87 g/t Ag is obtained,with 64.86% Cu and 59.79% Ag recovered.
Key concepts: Fineness, Metallurgy, Grinding, Smelting, Copper, Zinc, Zinc smelting, Materials science