The Influence of Constituents and MA Conditions on the Mechanical Properties of Ni3Si Intermetallic Compounds.
Nobushige Hiraishi, Kazutaka Asabe
Abstract
Open-access reader
Nobushige Hiraishi, Kazutaka Asabe
Abstract
Open-access reader
Ni3Si intermetallic compounds have an excellent corrosion resistance in sulphuricacid solution. However, production of these compounds was difficult because of poor ductility caused by formation of a very brittle phase. In order to suppress formation of the brittle phase, process conditions involving a mechanical alloying(MA) method have been investigated for the production of Ni3Si intermetallic compounds. First, fine Ni-Si composite powders prepared by the MA method were hot extruded. Then Ni3Si intermetallic compounds were obtained by a particular heat treatment. Influence of the constituents and the MA conditions on mechanical properties of the Ni3Si intermetallic compounds were investigated. As a result, in 13.1 mass%Si- 86.9 mass%Ni materials, tensile strength improved as MA time became longer, although the material had poor ductility. When the Si content was reduced below 13.1 mass%, the tensile strength improved and ductility increased. The critical Si content for achieving of ductility was 12.2 mass%Si.
OpenAlex reports 1 citations for this work. Citation counts describe recorded attention and do not establish research quality.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
Ni3Si intermetallic compounds have an excellent corrosion resistance in sulphuricacid solution. However, production of these compounds was difficult because of poor ductility caused by formation of a very brittle phase. In order to suppress formation of the brittle phase, process conditions involving a mechanical alloying(MA) method have been investigated for the production of Ni3Si intermetallic compounds. First, fine Ni-Si composite powders prepared by the MA method were hot extruded. Then Ni3Si intermetallic compounds were obtained by a particular heat treatment. Influence of the constituents and the MA conditions on mechanical properties of the Ni3Si intermetallic compounds were investigated. As a result, in 13.1 mass%Si- 86.9 mass%Ni materials, tensile strength improved as MA time became longer, although the material had poor ductility. When the Si content was reduced below 13.1 mass%, the tensile strength improved and ductility increased. The critical Si content for achieving of ductility was 12.2 mass%Si.
Key concepts: Intermetallic, Ductility (Earth science), Materials science, Brittleness, Ultimate tensile strength, Metallurgy, Phase (matter), Composite material