Outgassing Rate of the Copper-Plated Beam Tube for ISABELLE

H. C. Hseuh, E. F. Gaudet

Open full text 0 citations

Abstract

The ultrahigh vacuum system of the intersecting storage accelerator, ISABELLE, will consist of two interlaced rings of stainless steel beam tubes with a circumference 212 miles each. To obtain a good heat conduction during bakeout and to reduce the resistive wall instability during beam operation, a 1mm thick copper coating will be electroplated to the outer surface of this 1.5mm thick beam tube. To minimize the beam loss due to beam-gas collision, the pressure inside the beam tube is required to be 1 × 10-11 Torr (N2 equivalent) or less. To achieve this ultrahigh vacuum, the outgassing rate of the 304 LN stainlefs steel tubes has been reduced to ~1 × 10-13 Torr·l/cm2· sec by vacuum firing at 950°C for one hour. However, during acid-bath electroplating of copper, significant amount of hydrogen will be reintroduced and trapped in stainless steel which will substantially increase the outgassing rate (to ~2 × 10-12 Torr·l/cm2 sec). The outgassing characteristics of these copper-plated beam tubes are studied and discussed within the scope of diffusion and energy of activation. Methods to reduce the outgassing rate to an acceptable level (~l × 10-13 Torr·l/cm2·sec) are also given.

Open-access reader

About this research paper

What this paper is about

The ultrahigh vacuum system of the intersecting storage accelerator, ISABELLE, will consist of two interlaced rings of stainless steel beam tubes with a circumference 212 miles each. To obtain a good heat conduction during bakeout and to reduce the resistive wall instability during beam operation, a 1mm thick copper coating will be electroplated to the outer surface of this 1.5mm thick beam tube. To minimize the beam loss due to beam-gas collision, the pressure inside the beam tube is required to be 1 × 10-11 Torr (N2 equivalent) or less. To achieve this ultrahigh vacuum, the outgassing rate of the 304 LN stainlefs steel tubes has been reduced to ~1 × 10-13 Torr·l/cm2· sec by vacuum firing at 950°C for one hour. However, during acid-bath electroplating of copper, significant amount of hydrogen will be reintroduced and trapped in stainless steel which will substantially increase the outgassing rate (to ~2 × 10-12 Torr·l/cm2 sec). The outgassing characteristics of these copper-plated beam tubes are studied and discussed within the scope of diffusion and energy of activation. Methods to reduce the outgassing rate to an acceptable level (~l × 10-13 Torr·l/cm2·sec) are also given.

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

The ultrahigh vacuum system of the intersecting storage accelerator, ISABELLE, will consist of two interlaced rings of stainless steel beam tubes with a circumference 212 miles each. To obtain a good heat conduction during bakeout and to reduce the resistive wall instability during beam operation, a 1mm thick copper coating will be electroplated to the outer surface of this 1.5mm thick beam tube. To minimize the beam loss due to beam-gas collision, the pressure inside the beam tube is required to be 1 × 10-11 Torr (N2 equivalent) or less. To achieve this ultrahigh vacuum, the outgassing rate of the 304 LN stainlefs steel tubes has been reduced to ~1 × 10-13 Torr·l/cm2· sec by vacuum firing at 950°C for one hour. However, during acid-bath electroplating of copper, significant amount of hydrogen will be reintroduced and trapped in stainless steel which will substantially increase the outgassing rate (to ~2 × 10-12 Torr·l/cm2 sec). The outgassing characteristics of these copper-plated beam tubes are studied and discussed within the scope of diffusion and energy of activation. Methods to reduce the outgassing rate to an acceptable level (~l × 10-13 Torr·l/cm2·sec) are also given.

Key concepts: Outgassing, Torr, Materials science, Copper, Beam (structure), Tube (container), Electroplating, Hydrogen

Related papers

Back to paper searchBrowse research topicsOriginal source
Outgassing Rate of the Copper-Plated Beam Tube for ISABELLE — Research Paper | ScholarLens