Microtensile bond strengths of single-step self-etch adhesive systems to bovine dentin

Satoshi Uekusa, Keishi Tsubota, Motoka Tonegawa, Hiroaki Tsuchiya, Mika Iwasa, Ryo Kawamoto, Toshiki Takamizawa, Masashi Miyazaki

Open full text 18 citations

Abstract

The purpose of this study was to examine the microtensile bond strength of a single-step self-etch adhesive system (Clearfil tri-S Bond and One-Up Bond F Plus) to bovine dentin. Adhesive was applied to a flat dentin surface, and resin composite was bonded according to the manufacturers' instructions. After 24 h storage in distilled water at 37 degrees C, hourglass-shaped specimens were produced. These were subjected to microtensile bond strength testing at a cross-head speed of 1.0 mm/min. The results were analyzed using Student's t-test at a significance level of 0.05. Field-emission scanning electron microscopy (FE-SEM) observations of the fractured specimens and the adhesive-treated dentin surfaces were also conducted. The bond strength of Clearfil tri-S Bond was not significantly different from that of One-Up Bond F Plus, 41.1 +/- 10.1 versus 42.3 +/- 6.0 MPa. Mode of failure analysis for Clearfil tri-S Bond revealed an equal distribution between the three types of failure, and the predominant mode of failure was adhesive for One-Up Bond F Plus. FE-SEM observations of dentin to which adhesive had been applied revealed that the smear layer had been removed and the collagen fibers exposed.

Open-access reader

About this research paper

What this paper is about

The purpose of this study was to examine the microtensile bond strength of a single-step self-etch adhesive system (Clearfil tri-S Bond and One-Up Bond F Plus) to bovine dentin. Adhesive was applied to a flat dentin surface, and resin composite was bonded according to the manufacturers' instructions. After 24 h storage in distilled water at 37 degrees C, hourglass-shaped specimens were produced. These were subjected to microtensile bond strength testing at a cross-head speed of 1.0 mm/min. The results were analyzed using Student's t-test at a significance level of 0.05. Field-emission scanning electron microscopy (FE-SEM) observations of the fractured specimens and the adhesive-treated dentin surfaces were also conducted. The bond strength of Clearfil tri-S Bond was not significantly different from that of One-Up Bond F Plus, 41.1 +/- 10.1 versus 42.3 +/- 6.0 MPa. Mode of failure analysis for Clearfil tri-S Bond revealed an equal distribution between the three types of failure, and the predominant mode of failure was adhesive for One-Up Bond F Plus. FE-SEM observations of dentin to which adhesive had been applied revealed that the smear layer had been removed and the collagen fibers exposed.

Why it matters

OpenAlex reports 18 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

The purpose of this study was to examine the microtensile bond strength of a single-step self-etch adhesive system (Clearfil tri-S Bond and One-Up Bond F Plus) to bovine dentin. Adhesive was applied to a flat dentin surface, and resin composite was bonded according to the manufacturers' instructions. After 24 h storage in distilled water at 37 degrees C, hourglass-shaped specimens were produced. These were subjected to microtensile bond strength testing at a cross-head speed of 1.0 mm/min. The results were analyzed using Student's t-test at a significance level of 0.05. Field-emission scanning electron microscopy (FE-SEM) observations of the fractured specimens and the adhesive-treated dentin surfaces were also conducted. The bond strength of Clearfil tri-S Bond was not significantly different from that of One-Up Bond F Plus, 41.1 +/- 10.1 versus 42.3 +/- 6.0 MPa. Mode of failure analysis for Clearfil tri-S Bond revealed an equal distribution between the three types of failure, and the predominant mode of failure was adhesive for One-Up Bond F Plus. FE-SEM observations of dentin to which adhesive had been applied revealed that the smear layer had been removed and the collagen fibers exposed.

Key concepts: Dentin, Bond strength, Adhesive, Materials science, Single bond, Composite material, Distilled water, Smear layer