Properties of Sol-Gel Coating Film Synthesized from Nano Boehmite and Methyltrimethoxysilane
In Hye Myung, Myeong Sang Ahn, Dong Pil Kang
Abstract
In Hye Myung, Myeong Sang Ahn, Dong Pil Kang
Abstract
Several sol solutions were synthesized by using two kinds of nanosized boehmite and methyltrimethoxysilane (MTMS) according to the changing amount of MTMS at different reaction time. To understand their physical and chemical properties, sol-gel coating films were fabricated on glass. The sol solutions were prepared from boehmite of spherical shape (boehmite1)/MTMS and mixed boehmites of spherical and fibrous shapes (boehmite2)/MTMS. The soluble stability of boehmite1/MTMS was observed in the sol solution left for 24 h, however, that of boehmite2/MTMS was observed in the sol solution left for 48 h. The contact angle of sol-gel coating films from boehmite/MTMS increased with MTMS contents and reaction time. The films formed a flat surface with the increasing MTMS contents and decreasing reaction time. The electrical resistivity of films increased with MTMS contents. The thermal degradation of films occurred at approximately 400 oC.
OpenAlex reports 1 citations for this work. Citation counts describe recorded attention and do not establish research quality.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
Several sol solutions were synthesized by using two kinds of nanosized boehmite and methyltrimethoxysilane (MTMS) according to the changing amount of MTMS at different reaction time. To understand their physical and chemical properties, sol-gel coating films were fabricated on glass. The sol solutions were prepared from boehmite of spherical shape (boehmite1)/MTMS and mixed boehmites of spherical and fibrous shapes (boehmite2)/MTMS. The soluble stability of boehmite1/MTMS was observed in the sol solution left for 24 h, however, that of boehmite2/MTMS was observed in the sol solution left for 48 h. The contact angle of sol-gel coating films from boehmite/MTMS increased with MTMS contents and reaction time. The films formed a flat surface with the increasing MTMS contents and decreasing reaction time. The electrical resistivity of films increased with MTMS contents. The thermal degradation of films occurred at approximately 400 oC.
Key concepts: Methyltrimethoxysilane, Materials science, Sol-gel, Boehmite, Coating, Chemical engineering, Dip-coating, Composite material