2007Plasma Processes and PolymersOpen access

Properties of Pulsed Magnetron Sputtered TiO2 Coatings Grown under Different Magnetron Configurations and Power Deliver Modes

Y.N. Kok, Peter Kelly

Open full text 10 citations

Abstract

The mid-frequency (20–350 kHz) pulsed magnetron sputtering process has been reported as an enabling technology for the deposition of a wide range of commercially important coatings onto large area glass components. In this study, transparent titania (TiO2) coatings were deposited by reactive unbalanced magnetron sputtering in a Large Area rig built ‘in-house’ and designed to replicate an in-line coater. Deposition took place in continuous DC, pulsed DC (40, 100, 200 and 300 kHz) and AC (40 kHz) modes. The films were deposited under different magnetron configurations; single and dual planar magnetrons operated in conventional mode, and dual planar magnetrons operated in full-face erosion (FFE) mode. A calibration run was carried out for each setting to obtain the deposition rate. Then, a 1 µm thick coating was deposited onto float glass. During the sputtering process the substrates were reciprocated in a plane parallel with respect to the magnetron. The film properties were compared and assessed in terms of their structures, optical and mechanical properties using scanning electron microscopy (SEM), X-ray diffraction (XRD), spectrophotometry and nanoindentation testing. This paper compares the properties of TiO2 produced by DC, AC and pulsed DC magnetron sputtering using different magnetron configurations (static or FFE) and attempts to relate these properties to deposition parameters.

Open-access reader

About this research paper

What this paper is about

The mid-frequency (20–350 kHz) pulsed magnetron sputtering process has been reported as an enabling technology for the deposition of a wide range of commercially important coatings onto large area glass components. In this study, transparent titania (TiO2) coatings were deposited by reactive unbalanced magnetron sputtering in a Large Area rig built ‘in-house’ and designed to replicate an in-line coater. Deposition took place in continuous DC, pulsed DC (40, 100, 200 and 300 kHz) and AC (40 kHz) modes. The films were deposited under different magnetron configurations; single and dual planar magnetrons operated in conventional mode, and dual planar magnetrons operated in full-face erosion (FFE) mode. A calibration run was carried out for each setting to obtain the deposition rate. Then, a 1 µm thick coating was deposited onto float glass. During the sputtering process the substrates were reciprocated in a plane parallel with respect to the magnetron. The film properties were compared and assessed in terms of their structures, optical and mechanical properties using scanning electron microscopy (SEM), X-ray diffraction (XRD), spectrophotometry and nanoindentation testing. This paper compares the properties of TiO2 produced by DC, AC and pulsed DC magnetron sputtering using different magnetron configurations (static or FFE) and attempts to relate these properties to deposition parameters.

Why it matters

OpenAlex reports 10 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

The mid-frequency (20–350 kHz) pulsed magnetron sputtering process has been reported as an enabling technology for the deposition of a wide range of commercially important coatings onto large area glass components. In this study, transparent titania (TiO2) coatings were deposited by reactive unbalanced magnetron sputtering in a Large Area rig built ‘in-house’ and designed to replicate an in-line coater. Deposition took place in continuous DC, pulsed DC (40, 100, 200 and 300 kHz) and AC (40 kHz) modes. The films were deposited under different magnetron configurations; single and dual planar magnetrons operated in conventional mode, and dual planar magnetrons operated in full-face erosion (FFE) mode. A calibration run was carried out for each setting to obtain the deposition rate. Then, a 1 µm thick coating was deposited onto float glass. During the sputtering process the substrates were reciprocated in a plane parallel with respect to the magnetron. The film properties were compared and assessed in terms of their structures, optical and mechanical properties using scanning electron microscopy (SEM), X-ray diffraction (XRD), spectrophotometry and nanoindentation testing. This paper compares the properties of TiO2 produced by DC, AC and pulsed DC magnetron sputtering using different magnetron configurations (static or FFE) and attempts to relate these properties to deposition parameters.

Key concepts: Cavity magnetron, Materials science, Sputter deposition, Pulsed DC, High-power impulse magnetron sputtering, Scanning electron microscope, Deposition (geology), Nanoindentation

Related papers

Back to paper searchBrowse research topicsOriginal source
Properties of Pulsed Magnetron Sputtered TiO2 Coatings Grown under Different Magnetron Configurations and Power Deliver Modes — Research Paper | ScholarLens