2013•Petroleum Science and TechnologyRequires access

The Emulsification of Oxidized Wax With a Co/SBA-15 Catalyst

Honggen Peng, H. Zhao

Open publisher page 1 citations

Abstract

The mesoporous molecular sieve catalyst Co/SBA-15 was synthesized by two steps synthesis method, based on which oxidized wax was prepared. The emulsification of oxidized wax was carried out by employing Span-80, Tween-80, and stearic acid as compound emulsifier. The results showed that when the mass ratio of Span-80, Tween-80, and stearic acid was 5.5:3.6:0.9, emulsifying temperature was 75°C, emulsifying time was 55 min, emulsifier amount was 7.3%, and water consumption was 69.96%. The emulsion performance of oxidized wax was improved greatly compared with ordinary paraffins.

About this research paper

What this paper is about

The mesoporous molecular sieve catalyst Co/SBA-15 was synthesized by two steps synthesis method, based on which oxidized wax was prepared. The emulsification of oxidized wax was carried out by employing Span-80, Tween-80, and stearic acid as compound emulsifier. The results showed that when the mass ratio of Span-80, Tween-80, and stearic acid was 5.5:3.6:0.9, emulsifying temperature was 75°C, emulsifying time was 55 min, emulsifier amount was 7.3%, and water consumption was 69.96%. The emulsion performance of oxidized wax was improved greatly compared with ordinary paraffins.

Why it matters

OpenAlex reports 1 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

The mesoporous molecular sieve catalyst Co/SBA-15 was synthesized by two steps synthesis method, based on which oxidized wax was prepared. The emulsification of oxidized wax was carried out by employing Span-80, Tween-80, and stearic acid as compound emulsifier. The results showed that when the mass ratio of Span-80, Tween-80, and stearic acid was 5.5:3.6:0.9, emulsifying temperature was 75°C, emulsifying time was 55 min, emulsifier amount was 7.3%, and water consumption was 69.96%. The emulsion performance of oxidized wax was improved greatly compared with ordinary paraffins.

Key concepts: Wax, Stearic acid, Emulsion, Catalysis, Chemistry, Mesoporous material, Molecular sieve, Chemical engineering