2013Journal of the Korean Society for Heat TreatmentOpen access

Effects of Mo on the Mechanical Properties of Ductile Cast Iron with Cu Austempered at 380℃

G.Y. Kim

Open full text 0 citations

Abstract

In this study, we investigated effect of Mo addition on mechanical properties of Cu added ADI. Ductile cast iron specimens were austenitized at $900^{\circ}C$ for 150 min and then austempered at $380^{\circ}C$ for the various time periods from 15 min to 480 min. Mo added ADI had a higher volume fraction of retained austenite, and the volume fraction of retained austenite was determined by XRD analysis. As decreasing volume fraction of retained austenite, the elongation was also decreased as expected. But the UTS and yield strength were not decreased.

Open-access reader

About this research paper

What this paper is about

In this study, we investigated effect of Mo addition on mechanical properties of Cu added ADI. Ductile cast iron specimens were austenitized at $900^{\circ}C$ for 150 min and then austempered at $380^{\circ}C$ for the various time periods from 15 min to 480 min. Mo added ADI had a higher volume fraction of retained austenite, and the volume fraction of retained austenite was determined by XRD analysis. As decreasing volume fraction of retained austenite, the elongation was also decreased as expected. But the UTS and yield strength were not decreased.

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

In this study, we investigated effect of Mo addition on mechanical properties of Cu added ADI. Ductile cast iron specimens were austenitized at $900^{\circ}C$ for 150 min and then austempered at $380^{\circ}C$ for the various time periods from 15 min to 480 min. Mo added ADI had a higher volume fraction of retained austenite, and the volume fraction of retained austenite was determined by XRD analysis. As decreasing volume fraction of retained austenite, the elongation was also decreased as expected. But the UTS and yield strength were not decreased.

Key concepts: Austempering, Austenite, Volume fraction, Materials science, Elongation, Metallurgy, Cast iron, Volume (thermodynamics)

Related papers

Back to paper searchBrowse research topicsOriginal source
Effects of Mo on the Mechanical Properties of Ductile Cast Iron with Cu Austempered at 380℃ — Research Paper | ScholarLens