Preparation and Analysis of Kaolinite Intercalated by Potassium Acetate

Xiao Man Du, Qin Fu Liu, Hong Fei Cheng

Open publisher page 1 citations

Abstract

The kaolinite-potassium acetate composite was prepared by the immersion method. The intercalation composites were characterized by means of Scanning Electron Microscope (SEM), X-ray diffraction (XRD), Fourier transformation infrared (FT-IR) and High-resolution thermogravimetric analysis (HRTG). The results of XRD show that the intercalation of kaolinite by potassium acetate causes an increase of the basal spacing from 0.718 to 1.42nm. Thermal analysis shows the dehydroxylation of kaolinite decreased from 464 °C to 459.5 °C after intercalation of potassium acetate and three endotherms at 280, 323 and 459.5 °C attributed to the loss of water in the composite, potassium acetate and hydroxyl in the composite.

About this research paper

What this paper is about

The kaolinite-potassium acetate composite was prepared by the immersion method. The intercalation composites were characterized by means of Scanning Electron Microscope (SEM), X-ray diffraction (XRD), Fourier transformation infrared (FT-IR) and High-resolution thermogravimetric analysis (HRTG). The results of XRD show that the intercalation of kaolinite by potassium acetate causes an increase of the basal spacing from 0.718 to 1.42nm. Thermal analysis shows the dehydroxylation of kaolinite decreased from 464 °C to 459.5 °C after intercalation of potassium acetate and three endotherms at 280, 323 and 459.5 °C attributed to the loss of water in the composite, potassium acetate and hydroxyl in the composite.

Why it matters

OpenAlex reports 1 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

The kaolinite-potassium acetate composite was prepared by the immersion method. The intercalation composites were characterized by means of Scanning Electron Microscope (SEM), X-ray diffraction (XRD), Fourier transformation infrared (FT-IR) and High-resolution thermogravimetric analysis (HRTG). The results of XRD show that the intercalation of kaolinite by potassium acetate causes an increase of the basal spacing from 0.718 to 1.42nm. Thermal analysis shows the dehydroxylation of kaolinite decreased from 464 °C to 459.5 °C after intercalation of potassium acetate and three endotherms at 280, 323 and 459.5 °C attributed to the loss of water in the composite, potassium acetate and hydroxyl in the composite.

Key concepts: Intercalation (chemistry), Kaolinite, Potassium, Thermogravimetric analysis, Scanning electron microscope, Fourier transform infrared spectroscopy, Composite number, Thermal analysis

Related papers

Back to paper searchBrowse research topicsOriginal source
Preparation and Analysis of Kaolinite Intercalated by Potassium Acetate — Research Paper | ScholarLens