Molecular design and development of photoresists for ArF excimer laser lithography
Etsuo Hasegawa, Katsumi Maeda, Shigeyuki Iwasa
Abstract
Etsuo Hasegawa, Katsumi Maeda, Shigeyuki Iwasa
Abstract
Positive-tone and negative-tone resists for ArF excimer laser lithography are developed from novel polymers, which are called functionally-integrated polymers having polar alicyclic units. The fundamental unit of the polymers is an acrylate having a tetracyclododecane group with a carboxyl end group, which satisfies a lot of the requirements of ArF resists. A typical monomer is carboxy-tetracyclo[4.4.0.12,5.17,10]dodecyl methacrylate. In 1996, we established 0.15-µm “positive” line-and-space patterns at 21.8 mJ/cm2 using an ArF exposure system (0.55 numerical aperture), which meet the design rule requirement for fabricating 1-gigabit dynamic random access memories (DRAMs). This fundamental polymer unit has also been used to develop negative-tone resists for ArF lithography. In 1999, we also established 0.13-µm “negative” isolated line pattern at 7.1 mJ/cm2 using an ArF exposure system which fulfills the design rule requirement for logic circuits combined with gigabit DRAMs. Copyright © 2000 John Wiley & Sons, Ltd.
OpenAlex reports 9 citations for this work. Citation counts describe recorded attention and do not establish research quality.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
Positive-tone and negative-tone resists for ArF excimer laser lithography are developed from novel polymers, which are called functionally-integrated polymers having polar alicyclic units. The fundamental unit of the polymers is an acrylate having a tetracyclododecane group with a carboxyl end group, which satisfies a lot of the requirements of ArF resists. A typical monomer is carboxy-tetracyclo[4.4.0.12,5.17,10]dodecyl methacrylate. In 1996, we established 0.15-µm “positive” line-and-space patterns at 21.8 mJ/cm2 using an ArF exposure system (0.55 numerical aperture), which meet the design rule requirement for fabricating 1-gigabit dynamic random access memories (DRAMs). This fundamental polymer unit has also been used to develop negative-tone resists for ArF lithography. In 1999, we also established 0.13-µm “negative” isolated line pattern at 7.1 mJ/cm2 using an ArF exposure system which fulfills the design rule requirement for logic circuits combined with gigabit DRAMs. Copyright © 2000 John Wiley & Sons, Ltd.
Key concepts: Resist, Lithography, Excimer laser, Photolithography, Materials science, Polymer, Masking (illustration), Optoelectronics