2015Applied Physics LettersRequires access

Energy-band diagram configuration of Al2O3/oxygen-terminated p-diamond metal-oxide-semiconductor

Aurélien Maréchal, Manuela Aoukar, C. Vallée, C. Rivière, David Eon, Julien Pernot, E. Gheeraert

Open publisher page 42 citations

Abstract

Diamond metal-oxide-semiconductor capacitors were prepared using atomic layer deposition at 250 °C of Al2O3 on oxygen-terminated boron doped (001) diamond. Their electrical properties were investigated in terms of capacitance and current versus voltage measurements. Performing X-ray photoelectron spectroscopy based on the measured core level energies and valence band maxima, the interfacial energy band diagram configuration of the Al2O3/O-diamond is established. The band diagram alignment is concluded to be of type I with valence band offset ΔEv of 1.34 ± 0.2 eV and conduction band offset ΔEc of 0.56 ± 0.2 eV considering an Al2O3 energy band gap of 7.4 eV. The agreement with electrical measurement and the ability to perform a MOS transistor are discussed.

About this research paper

What this paper is about

Diamond metal-oxide-semiconductor capacitors were prepared using atomic layer deposition at 250 °C of Al2O3 on oxygen-terminated boron doped (001) diamond. Their electrical properties were investigated in terms of capacitance and current versus voltage measurements. Performing X-ray photoelectron spectroscopy based on the measured core level energies and valence band maxima, the interfacial energy band diagram configuration of the Al2O3/O-diamond is established. The band diagram alignment is concluded to be of type I with valence band offset ΔEv of 1.34 ± 0.2 eV and conduction band offset ΔEc of 0.56 ± 0.2 eV considering an Al2O3 energy band gap of 7.4 eV. The agreement with electrical measurement and the ability to perform a MOS transistor are discussed.

Why it matters

OpenAlex reports 42 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Diamond metal-oxide-semiconductor capacitors were prepared using atomic layer deposition at 250 °C of Al2O3 on oxygen-terminated boron doped (001) diamond. Their electrical properties were investigated in terms of capacitance and current versus voltage measurements. Performing X-ray photoelectron spectroscopy based on the measured core level energies and valence band maxima, the interfacial energy band diagram configuration of the Al2O3/O-diamond is established. The band diagram alignment is concluded to be of type I with valence band offset ΔEv of 1.34 ± 0.2 eV and conduction band offset ΔEc of 0.56 ± 0.2 eV considering an Al2O3 energy band gap of 7.4 eV. The agreement with electrical measurement and the ability to perform a MOS transistor are discussed.

Key concepts: Band diagram, Diamond, Band offset, Materials science, Semiconductor, Band gap, Oxide, Semimetal

Related papers

Back to paper searchBrowse research topicsOriginal source
Energy-band diagram configuration of Al2O3/oxygen-terminated p-diamond metal-oxide-semiconductor — Research Paper | ScholarLens