NBTI enhancement by nitrogen incorporation into ultrathin gate oxide for 0.10-μm gate CMOS generation

N. Kimizuka, Keiko Yamaguchi, K. Imai, T. Iizuka, C.T. Liu, Robert C. Keller, T. Horiuchi

Open publisher page 139 citations

Abstract

We investigated the degradation of device reliability due to Negative Bias Temperature Instability (NBTI) of PMOSFET with ultrathin gate oxide. It was experimentally demonstrated that the chemical reactions at the gate oxide/substrate interface and/or diffusion of hydrogen related species are the major cause of the NBTI. We also found that nitridation of gate oxide enhances NBTI. In order to suppress the NBTI, the density of hydrogen terminated silicon bond at the interface needs to be minimized. Thus, the concentration of nitrogen in thin gate oxide has to be optimized in terms of the reliability reduction due to NBTI.

About this research paper

What this paper is about

We investigated the degradation of device reliability due to Negative Bias Temperature Instability (NBTI) of PMOSFET with ultrathin gate oxide. It was experimentally demonstrated that the chemical reactions at the gate oxide/substrate interface and/or diffusion of hydrogen related species are the major cause of the NBTI. We also found that nitridation of gate oxide enhances NBTI. In order to suppress the NBTI, the density of hydrogen terminated silicon bond at the interface needs to be minimized. Thus, the concentration of nitrogen in thin gate oxide has to be optimized in terms of the reliability reduction due to NBTI.

Why it matters

OpenAlex reports 139 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

We investigated the degradation of device reliability due to Negative Bias Temperature Instability (NBTI) of PMOSFET with ultrathin gate oxide. It was experimentally demonstrated that the chemical reactions at the gate oxide/substrate interface and/or diffusion of hydrogen related species are the major cause of the NBTI. We also found that nitridation of gate oxide enhances NBTI. In order to suppress the NBTI, the density of hydrogen terminated silicon bond at the interface needs to be minimized. Thus, the concentration of nitrogen in thin gate oxide has to be optimized in terms of the reliability reduction due to NBTI.

Key concepts: Negative-bias temperature instability, Materials science, Gate oxide, CMOS, Oxide, Optoelectronics, Reliability (semiconductor), Degradation (telecommunications)