2012•DOAJ (DOAJ: Directory of Open Access Journals)Open access

Effects of ABS-g-MAH on the properties of Nylon 6/ABS alloy

Wang Chao, 李迎春, 郭晓晨, 郑佳星, 张少峰

Open full text 0 citations

Abstract

The alloy of Nylon 6/acrylonitrile-butadiene-styrene(ABS)was used for a compatibilizer to generate the maleic anhydride(ABS-g-MAH),in which the proportion of PA6/ABS is 90/10.The results of the mechanical tests show that when the content of ABS-g-MAH is 20%,the impact strength of the alloy with the compatibilizer increased by around 41%,compared with that of the PA6/ABS alloy;Besides,the tensile strength has been significantly improved.Furthermore,in accordance with the dynamic mechanical analysis,α relaxation temperature of Nylon 6 has raised from 70 ℃ to 110 ℃ with the addition of ABS and ABS-g-MAH;moreover,and the obvious relaxations of β and γ occur at about 60 ℃ and-60 ℃,respectively.It can be seen from the scanning electron microscope(SEM)photographs that the compatibility has been improved through the addition of ABS-g-MAH.The water absorption of Nylon 6 has also been improved by the addition of ABS and ABS-g-MAH.When the content of ABS-g-MAH is 10%,the water absorption of the alloy will fall by 50%.

About this research paper

What this paper is about

The alloy of Nylon 6/acrylonitrile-butadiene-styrene(ABS)was used for a compatibilizer to generate the maleic anhydride(ABS-g-MAH),in which the proportion of PA6/ABS is 90/10.The results of the mechanical tests show that when the content of ABS-g-MAH is 20%,the impact strength of the alloy with the compatibilizer increased by around 41%,compared with that of the PA6/ABS alloy;Besides,the tensile strength has been significantly improved.Furthermore,in accordance with the dynamic mechanical analysis,α relaxation temperature of Nylon 6 has raised from 70 ℃ to 110 ℃ with the addition of ABS and ABS-g-MAH;moreover,and the obvious relaxations of β and γ occur at about 60 ℃ and-60 ℃,respectively.It can be seen from the scanning electron microscope(SEM)photographs that the compatibility has been improved through the addition of ABS-g-MAH.The water absorption of Nylon 6 has also been improved by the addition of ABS and ABS-g-MAH.When the content of ABS-g-MAH is 10%,the water absorption of the alloy will fall by 50%.

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

The alloy of Nylon 6/acrylonitrile-butadiene-styrene(ABS)was used for a compatibilizer to generate the maleic anhydride(ABS-g-MAH),in which the proportion of PA6/ABS is 90/10.The results of the mechanical tests show that when the content of ABS-g-MAH is 20%,the impact strength of the alloy with the compatibilizer increased by around 41%,compared with that of the PA6/ABS alloy;Besides,the tensile strength has been significantly improved.Furthermore,in accordance with the dynamic mechanical analysis,α relaxation temperature of Nylon 6 has raised from 70 ℃ to 110 ℃ with the addition of ABS and ABS-g-MAH;moreover,and the obvious relaxations of β and γ occur at about 60 ℃ and-60 ℃,respectively.It can be seen from the scanning electron microscope(SEM)photographs that the compatibility has been improved through the addition of ABS-g-MAH.The water absorption of Nylon 6 has also been improved by the addition of ABS and ABS-g-MAH.When the content of ABS-g-MAH is 10%,the water absorption of the alloy will fall by 50%.

Key concepts: Alloy, Materials science, Composite material

Related papers

Back to paper searchBrowse research topicsOriginal source
Effects of ABS-g-MAH on the properties of Nylon 6/ABS alloy — Research Paper | ScholarLens