EFFECT OF ACID-TREATMENT ON DENTIN BONDING
Young-Kyong Kim, Sung Kyo Kim, Jin-Hoon Park
Abstract
Young-Kyong Kim, Sung Kyo Kim, Jin-Hoon Park
Abstract
The purpose of this study was to evaluate the effect of various acid treatments on dentin bonding. Freshly extracted human teeth were uprightly embedded in self curing acrylic resin, and their occlusal surfaces were grinded to expose flat dentin surfaces. The specimens were divided into 4 groups. Specimens of one group were not treated so as to be a control and those of the other three groups were threated with 10% polyacrylic acid, 10% phosphoric acid, and 10-3 solution(10% citric acid/3% ferric chloride) respectively. Primer, bonding resin and composite resin were applied over the treated dentin surfaces sequentially. All specimens were stored in distilled water for 24 hours, then the tensile bond strength was measured and the treated dentin surfaces and fracured dentin surfaces were examined under a scanning electron microscope. The results were as follows: Bond strengths of acid-treated groups were higher than those of the untreated group. In the acid-treated groups, bond strength was found to be the highest in the 10-3 solution group followed by the 10% phosphoric acid group and the 10% polyacrylic acid group(P
A significance statement is not available in the OpenAlex record.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
The purpose of this study was to evaluate the effect of various acid treatments on dentin bonding. Freshly extracted human teeth were uprightly embedded in self curing acrylic resin, and their occlusal surfaces were grinded to expose flat dentin surfaces. The specimens were divided into 4 groups. Specimens of one group were not treated so as to be a control and those of the other three groups were threated with 10% polyacrylic acid, 10% phosphoric acid, and 10-3 solution(10% citric acid/3% ferric chloride) respectively. Primer, bonding resin and composite resin were applied over the treated dentin surfaces sequentially. All specimens were stored in distilled water for 24 hours, then the tensile bond strength was measured and the treated dentin surfaces and fracured dentin surfaces were examined under a scanning electron microscope. The results were as follows: Bond strengths of acid-treated groups were higher than those of the untreated group. In the acid-treated groups, bond strength was found to be the highest in the 10-3 solution group followed by the 10% phosphoric acid group and the 10% polyacrylic acid group(P
Key concepts: Phosphoric acid, Dentin, Polyacrylic acid, Citric acid, Distilled water, Bond strength, Chemistry, Nuclear chemistry