1996Journal of the Korean Society of Civil EngineersRequires access

A Study on Strength Characteristics of High Strength Concrete Containing Ground Granulated Blast-Furnace Slag

Han-Young Moon, Yun-Wang Choi

Open publisher page 0 citations

Abstract

High strength concrete has high heat of hydration and poor workability before setting resulted from significant slump loss due to a large amount of cement content and low water cement ratio.'Results of this study showed that properties of concrete containin GGBF(ground granulated blast-furnace) slag varying fineness, GGBF slag-cement ratio, age and cement content are slightly different from those of conventional high strength concrete. The maximum compressive strength at age of 28 days was . In addition, compressive strength, tensile strength and elastic modulus of concrete made with GGBF slag 30% replacement cement showed higher value than that of concrete not containing GGBF slag.

About this research paper

What this paper is about

High strength concrete has high heat of hydration and poor workability before setting resulted from significant slump loss due to a large amount of cement content and low water cement ratio.'Results of this study showed that properties of concrete containin GGBF(ground granulated blast-furnace) slag varying fineness, GGBF slag-cement ratio, age and cement content are slightly different from those of conventional high strength concrete. The maximum compressive strength at age of 28 days was . In addition, compressive strength, tensile strength and elastic modulus of concrete made with GGBF slag 30% replacement cement showed higher value than that of concrete not containing GGBF slag.

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

High strength concrete has high heat of hydration and poor workability before setting resulted from significant slump loss due to a large amount of cement content and low water cement ratio.'Results of this study showed that properties of concrete containin GGBF(ground granulated blast-furnace) slag varying fineness, GGBF slag-cement ratio, age and cement content are slightly different from those of conventional high strength concrete. The maximum compressive strength at age of 28 days was . In addition, compressive strength, tensile strength and elastic modulus of concrete made with GGBF slag 30% replacement cement showed higher value than that of concrete not containing GGBF slag.

Key concepts: Fineness, Ground granulated blast-furnace slag, Compressive strength, Cement, Materials science, Slump, Slag (welding), Ultimate tensile strength

Related papers

Back to paper searchBrowse research topicsOriginal source
A Study on Strength Characteristics of High Strength Concrete Containing Ground Granulated Blast-Furnace Slag — Research Paper | ScholarLens