2005Journal of the Korean Wood Science and TechnologyRequires access

Improvement of Drying Schedule for Domestic Red Pine Lumber

Hyoung-Woo Lee, Kyung‐Yong Kim

Open publisher page 0 citations

Abstract

This experiment was carried out for the improvement of drying schedules for 50 mm-thick Japanese red pine (Pinus densiflora Sieb. et Zucc.) lumber. Drying rates were analyzed comparatively after drying to 15% of final moisture content through the applications of conventional kiln drying schedule, time schedule, continuously rising temperature schedule, and drying rate schedule. As results drying rate of 50 mm-thick red pine lumber was 0.53%/hr with conventional kiln drying schedule, 0.9%/hr with time schedule, 2.29%/hr with continuously rising temperature schedule, and 1.52%/hr with drying rate schedule, respectively.

About this research paper

What this paper is about

This experiment was carried out for the improvement of drying schedules for 50 mm-thick Japanese red pine (Pinus densiflora Sieb. et Zucc.) lumber. Drying rates were analyzed comparatively after drying to 15% of final moisture content through the applications of conventional kiln drying schedule, time schedule, continuously rising temperature schedule, and drying rate schedule. As results drying rate of 50 mm-thick red pine lumber was 0.53%/hr with conventional kiln drying schedule, 0.9%/hr with time schedule, 2.29%/hr with continuously rising temperature schedule, and 1.52%/hr with drying rate schedule, respectively.

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

This experiment was carried out for the improvement of drying schedules for 50 mm-thick Japanese red pine (Pinus densiflora Sieb. et Zucc.) lumber. Drying rates were analyzed comparatively after drying to 15% of final moisture content through the applications of conventional kiln drying schedule, time schedule, continuously rising temperature schedule, and drying rate schedule. As results drying rate of 50 mm-thick red pine lumber was 0.53%/hr with conventional kiln drying schedule, 0.9%/hr with time schedule, 2.29%/hr with continuously rising temperature schedule, and 1.52%/hr with drying rate schedule, respectively.

Key concepts: Pinus densiflora, Schedule, Kiln, Wood drying, Red pine, Pulp and paper industry, Water content, Moisture

Related papers

Back to paper searchBrowse research topicsOriginal source
Improvement of Drying Schedule for Domestic Red Pine Lumber — Research Paper | ScholarLens