Charpy and Izod Method Impak Strength Analysis on ST 37 Steel with Temperature Variations
Eka Putra Dairi Boangmanalu, Angga Bahri Pratama, Al Qadry, Jandri Fan HT Saragi, Franklin Taruyun Hudeardo Sinaga
Abstract
Open-access reader
Eka Putra Dairi Boangmanalu, Angga Bahri Pratama, Al Qadry, Jandri Fan HT Saragi, Franklin Taruyun Hudeardo Sinaga
Abstract
Open-access reader
This research is impact testing using the Charpy and Izod methods, temperature variations of 1500 C, 2500 C and raw material as the research variable. The results of the Charpy test with a variation of 150 0C obtained a maximum absorbed energy of 97.65 J, with an impact value of 0.222 J/mm2. Then the maximum energy absorbed through testing at a temperature of 2500C is 78.28 Joules and the impact value is 0.177 J/mm2. Furthermore, the raw material test results showed that the maximum energy absorbed was 145.96 J with an impact value of 0.330 J/mm2. Izod testing with a temperature of 1500C obtained a maximum absorbed energy of 60.94 J with an impact value of 0.101 J/mm2. Furthermore, the maximum energy absorbed at a temperature of 2500C is 36.83 Joules and the impact value is 0.061 J/mm2. The raw material test results show that the maximum energy that can be absorbed is 80.53 J with an impact price of 0.133 J/mm2
OpenAlex reports 1 citations for this work. Citation counts describe recorded attention and do not establish research quality.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
This research is impact testing using the Charpy and Izod methods, temperature variations of 1500 C, 2500 C and raw material as the research variable. The results of the Charpy test with a variation of 150 0C obtained a maximum absorbed energy of 97.65 J, with an impact value of 0.222 J/mm2. Then the maximum energy absorbed through testing at a temperature of 2500C is 78.28 Joules and the impact value is 0.177 J/mm2. Furthermore, the raw material test results showed that the maximum energy absorbed was 145.96 J with an impact value of 0.330 J/mm2. Izod testing with a temperature of 1500C obtained a maximum absorbed energy of 60.94 J with an impact value of 0.101 J/mm2. Furthermore, the maximum energy absorbed at a temperature of 2500C is 36.83 Joules and the impact value is 0.061 J/mm2. The raw material test results show that the maximum energy that can be absorbed is 80.53 J with an impact price of 0.133 J/mm2
Key concepts: Charpy impact test, Izod impact strength test, Impact energy, Materials science, Raw material, Composite material, Toughness, Ultimate tensile strength