2023Jurnal Talenta SipilOpen access

Pengaruh Penambahan Aditif Sikament-Ln terhadap Kuat Tekan Beton Mutu Tinggi dengan Variasi Nilai Slump

Ibrahim Ibrahim, Kosim Kosim, Firdha Razhanah, Reynaldy Aji Nugraha, R. Reza Fahruddin

Open full text 0 citations

Abstract

High-strength concrete listed in SNI 03-6468-2000 concrete is defined as concrete having the required compressive strength of fc'≥ 41 Mpa. From this study, data obtained from the compressive strength of concrete at the age of 28 days as follows: the value of the normal concrete compressive strength of 41.72 MPa, the compressive strength of the Sikament-ln mixture of 0.6% slump 5 of 45.65 MPa, the compressive strength of the Sikament-mixed concrete. -ln 1% slump 6 of 47,38 MPa, compressive strength of mixed concrete Sikament-ln 1.4% slump 7 of 44.20 MPa, compressive strength of mixed concrete of Sikament-ln 1.8% slump 8 of 45.65 MPa 38 ,65MPa. It can be seen from the results of this study that the ideal compressive strength is the compressive strength of the Sikament-ln mixture of 1% slump 6 this is because the compressive strength value is much greater than the compressive strength without the Sikament-ln mixture.

Open-access reader

About this research paper

What this paper is about

High-strength concrete listed in SNI 03-6468-2000 concrete is defined as concrete having the required compressive strength of fc'≥ 41 Mpa. From this study, data obtained from the compressive strength of concrete at the age of 28 days as follows: the value of the normal concrete compressive strength of 41.72 MPa, the compressive strength of the Sikament-ln mixture of 0.6% slump 5 of 45.65 MPa, the compressive strength of the Sikament-mixed concrete. -ln 1% slump 6 of 47,38 MPa, compressive strength of mixed concrete Sikament-ln 1.4% slump 7 of 44.20 MPa, compressive strength of mixed concrete of Sikament-ln 1.8% slump 8 of 45.65 MPa 38 ,65MPa. It can be seen from the results of this study that the ideal compressive strength is the compressive strength of the Sikament-ln mixture of 1% slump 6 this is because the compressive strength value is much greater than the compressive strength without the Sikament-ln mixture.

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

High-strength concrete listed in SNI 03-6468-2000 concrete is defined as concrete having the required compressive strength of fc'≥ 41 Mpa. From this study, data obtained from the compressive strength of concrete at the age of 28 days as follows: the value of the normal concrete compressive strength of 41.72 MPa, the compressive strength of the Sikament-ln mixture of 0.6% slump 5 of 45.65 MPa, the compressive strength of the Sikament-mixed concrete. -ln 1% slump 6 of 47,38 MPa, compressive strength of mixed concrete Sikament-ln 1.4% slump 7 of 44.20 MPa, compressive strength of mixed concrete of Sikament-ln 1.8% slump 8 of 45.65 MPa 38 ,65MPa. It can be seen from the results of this study that the ideal compressive strength is the compressive strength of the Sikament-ln mixture of 1% slump 6 this is because the compressive strength value is much greater than the compressive strength without the Sikament-ln mixture.

Key concepts: Compressive strength, Slump, Materials science, Composite material, Concrete slump test, Geotechnical engineering, Geology

Related papers

Back to paper searchBrowse research topicsOriginal source
Pengaruh Penambahan Aditif Sikament-Ln terhadap Kuat Tekan Beton Mutu Tinggi dengan Variasi Nilai Slump — Research Paper | ScholarLens