2023NanoscaleOpen access

Built-in tensile strain dependence on the lateral size of monolayer MoS 2 synthesized by liquid precursor chemical vapor deposition

L. Seravalli, F. Esposito, Matteo Bosi, Lucrezia Aversa, Giovanna Trevisi, Roberto Verucchi, L. Lazzarini, Francesca Rossi, Filippo Fabbri

Open full text 24 citations

Abstract

/Si substrate by liquid precursor chemical vapor deposition, is mainly dependent on the size of the monolayer. In fact, we identify a critical size equal to 20 μm, from which the built-in strain increases drastically. The built-in strain is the maximum for a 60 μm sized monolayer, leading to 1.2% tensile strain with a partial release of strain close to the monolayer triangular vertexes due to the formation of nanocracks. These findings also imply that the standard method for evaluation of the number of layers based on the Raman mode separation can become unreliable for highly strained monolayers with a lateral size above 20 μm.

Open-access reader

About this research paper

What this paper is about

/Si substrate by liquid precursor chemical vapor deposition, is mainly dependent on the size of the monolayer. In fact, we identify a critical size equal to 20 μm, from which the built-in strain increases drastically. The built-in strain is the maximum for a 60 μm sized monolayer, leading to 1.2% tensile strain with a partial release of strain close to the monolayer triangular vertexes due to the formation of nanocracks. These findings also imply that the standard method for evaluation of the number of layers based on the Raman mode separation can become unreliable for highly strained monolayers with a lateral size above 20 μm.

Why it matters

OpenAlex reports 24 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

/Si substrate by liquid precursor chemical vapor deposition, is mainly dependent on the size of the monolayer. In fact, we identify a critical size equal to 20 μm, from which the built-in strain increases drastically. The built-in strain is the maximum for a 60 μm sized monolayer, leading to 1.2% tensile strain with a partial release of strain close to the monolayer triangular vertexes due to the formation of nanocracks. These findings also imply that the standard method for evaluation of the number of layers based on the Raman mode separation can become unreliable for highly strained monolayers with a lateral size above 20 μm.

Key concepts: Monolayer, Molybdenum disulfide, Chemical vapor deposition, Materials science, Raman spectroscopy, Strain (injury), Tensile strain, Substrate (aquarium)

Related papers

Back to paper searchBrowse research topicsOriginal source
Built-in tensile strain dependence on the lateral size of monolayer MoS 2 synthesized by liquid precursor chemical vapor deposition — Research Paper | ScholarLens