Abstract The modified nanosilica (mNS), acrylonitrile-butadiene rubber (NBR), and ethylene-propylene-diene monomer (EPDM) nanocomposite was created. The 70/30 EPDM/NBR and 0–10 parts per hundred rubber (phr) of mNS were mixed on a two-roll mill. The impact of mNS on compression set, mole percent uptake (MPU), cure characteristics (scorch and optimal cure time, cure rate index, maximum torque, minimum torque, and torque difference) and mechanical properties (tensile and tear strength, hardness, elongation at break, rebound resilience, and abrasion resistance) of the composites were investigated and discussed. The surface morphology of tensile-fractured EPDM/NBR rubber-mNS was investigated using FESEM. The material's tensile strength, 100% modulus, tear strength, hardness, and abrasion resistance were all improved with an increase in mNS concentration, but rebound resilience and elongation at break were decreased.
A significance statement is not available in the OpenAlex record.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
Abstract The modified nanosilica (mNS), acrylonitrile-butadiene rubber (NBR), and ethylene-propylene-diene monomer (EPDM) nanocomposite was created. The 70/30 EPDM/NBR and 0–10 parts per hundred rubber (phr) of mNS were mixed on a two-roll mill. The impact of mNS on compression set, mole percent uptake (MPU), cure characteristics (scorch and optimal cure time, cure rate index, maximum torque, minimum torque, and torque difference) and mechanical properties (tensile and tear strength, hardness, elongation at break, rebound resilience, and abrasion resistance) of the composites were investigated and discussed. The surface morphology of tensile-fractured EPDM/NBR rubber-mNS was investigated using FESEM. The material's tensile strength, 100% modulus, tear strength, hardness, and abrasion resistance were all improved with an increase in mNS concentration, but rebound resilience and elongation at break were decreased.
Key concepts: Tear resistance, Compression set, Materials science, Ultimate tensile strength, Composite material, Natural rubber, Elongation, Resilience (materials science)