2023Journal of Nuclear MaterialsOpen access

Mechanical behavior of high-Ni/high-Mn Barsebäck 2 reactor pressure vessel welds after 28 years of operation

Sebastian Lindqvist, Alex Norrgård, Pentti Arffman, Noora Hytönen, Jari Lydman, Pål Efsing, Siddharth Suman, Pekka Nevasmaa

Open full text 10 citations

Abstract

To assess long-term operation of the reactor pressure vessel (RPV), surveillance programs are applied for periodic monitoring and prediction of the aging of the mechanical properties due to irradiation and thermal embrittlement. In literature, there are limited data sets to compare the results from the surveillance program to the aging of the RPV. In this work, the tensile and impact toughness properties of the high-Ni, high-Mn welds from decommissioned Barsebäck 2 RPV are characterized. The results indicate that the surveillance program describes sufficiently the aging of the RPV welds. Differences in mechanical properties of the welds from various regions are explained by variations in post-weld heat treatment. The synergetic effect of Ni and Mn on embrittlement appears not to result at low fluences in a significant difference in the embrittlement rate when compared to ASTM E900 embrittlement trend curve prediction.

About this research paper

What this paper is about

To assess long-term operation of the reactor pressure vessel (RPV), surveillance programs are applied for periodic monitoring and prediction of the aging of the mechanical properties due to irradiation and thermal embrittlement. In literature, there are limited data sets to compare the results from the surveillance program to the aging of the RPV. In this work, the tensile and impact toughness properties of the high-Ni, high-Mn welds from decommissioned Barsebäck 2 RPV are characterized. The results indicate that the surveillance program describes sufficiently the aging of the RPV welds. Differences in mechanical properties of the welds from various regions are explained by variations in post-weld heat treatment. The synergetic effect of Ni and Mn on embrittlement appears not to result at low fluences in a significant difference in the embrittlement rate when compared to ASTM E900 embrittlement trend curve prediction.

Why it matters

OpenAlex reports 10 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

To assess long-term operation of the reactor pressure vessel (RPV), surveillance programs are applied for periodic monitoring and prediction of the aging of the mechanical properties due to irradiation and thermal embrittlement. In literature, there are limited data sets to compare the results from the surveillance program to the aging of the RPV. In this work, the tensile and impact toughness properties of the high-Ni, high-Mn welds from decommissioned Barsebäck 2 RPV are characterized. The results indicate that the surveillance program describes sufficiently the aging of the RPV welds. Differences in mechanical properties of the welds from various regions are explained by variations in post-weld heat treatment. The synergetic effect of Ni and Mn on embrittlement appears not to result at low fluences in a significant difference in the embrittlement rate when compared to ASTM E900 embrittlement trend curve prediction.

Key concepts: Embrittlement, Reactor pressure vessel, Materials science, Welding, Pressure vessel, Metallurgy, Toughness, Ultimate tensile strength