2023Key engineering materialsOpen access

Corrosion Behavior of Hastelloy C-276 in Hydrochloric and Sulfuric Acid

Sri Hastuty, Anang Widiatmoko, Toto Sudiro, Muhammad Awwaluddin, Poppy Puspitasari

Open full text 2 citations

Abstract

This research was conducted to determine the corrosion rate by varying the concentration of the solution against hydrochloric acid and sulfuric acid. The method used is open circuit potential (OCP) and Tafel plot. Based on the research conducted, Hastelloy C-276 was more prone to get oxidized in sulfuric acid rather than hydrochloric acid. It can be seen from the OCP value of sulfuric acid was much more negative than that of hydrochloric acid as of-1.5 V for 0.5 M sulfuric acid and-0.2 V for hydrochloric acid. The corrosion rate of Hastelloy C-276 in sulfuric acid was also higher compared to same alloy in hydrochloric acid. At the most concentrated solution, 0.5 M, the corrosion rate of sulfuric acid reached 0.39 mmpy and as for corrosion cate in hydrochloric acid, only at 0.16 mmpy. It is thought that there was a difference of passive film composition for both solutions. Keywords: Hastelloy C-276, Corrosion, Hydrochloric acid, Sulfuric acid.

About this research paper

What this paper is about

This research was conducted to determine the corrosion rate by varying the concentration of the solution against hydrochloric acid and sulfuric acid. The method used is open circuit potential (OCP) and Tafel plot. Based on the research conducted, Hastelloy C-276 was more prone to get oxidized in sulfuric acid rather than hydrochloric acid. It can be seen from the OCP value of sulfuric acid was much more negative than that of hydrochloric acid as of-1.5 V for 0.5 M sulfuric acid and-0.2 V for hydrochloric acid. The corrosion rate of Hastelloy C-276 in sulfuric acid was also higher compared to same alloy in hydrochloric acid. At the most concentrated solution, 0.5 M, the corrosion rate of sulfuric acid reached 0.39 mmpy and as for corrosion cate in hydrochloric acid, only at 0.16 mmpy. It is thought that there was a difference of passive film composition for both solutions. Keywords: Hastelloy C-276, Corrosion, Hydrochloric acid, Sulfuric acid.

Why it matters

OpenAlex reports 2 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

This research was conducted to determine the corrosion rate by varying the concentration of the solution against hydrochloric acid and sulfuric acid. The method used is open circuit potential (OCP) and Tafel plot. Based on the research conducted, Hastelloy C-276 was more prone to get oxidized in sulfuric acid rather than hydrochloric acid. It can be seen from the OCP value of sulfuric acid was much more negative than that of hydrochloric acid as of-1.5 V for 0.5 M sulfuric acid and-0.2 V for hydrochloric acid. The corrosion rate of Hastelloy C-276 in sulfuric acid was also higher compared to same alloy in hydrochloric acid. At the most concentrated solution, 0.5 M, the corrosion rate of sulfuric acid reached 0.39 mmpy and as for corrosion cate in hydrochloric acid, only at 0.16 mmpy. It is thought that there was a difference of passive film composition for both solutions. Keywords: Hastelloy C-276, Corrosion, Hydrochloric acid, Sulfuric acid.

Key concepts: Sulfuric acid, Hydrochloric acid, Corrosion, Tafel equation, Materials science, Inorganic chemistry, Metallurgy, Chemistry

Related papers

Back to paper searchBrowse research topicsOriginal source
Corrosion Behavior of Hastelloy C-276 in Hydrochloric and Sulfuric Acid — Research Paper | ScholarLens