2022•Macromolecular Rapid CommunicationsRequires access

Synthesis and Characterization of a New Copolymer Consisting of Polyamide 1210 and Reactive Phosphorus−Nitrogen Flame‐Retardant

Lizheng Qin, Yang Zhou, Shun Gong, Shikun Zhao, Zhiwen Cao, Jianping Deng, Kai Pan

Open publisher page 18 citations

Abstract

The thermal stability and reactivity of organophosphorus flame-retardants play a critical role in synthesizing copolymerized flame-retardant polyamides. Herein, this work successfully synthesizes a flame-retardant CEPPA-DDA salt (CDS) with both good thermal stability and high reactivity by reacting 2-carboxyethyl phenyl phosphonic acid (CEPPA) with 1,12-dodecanediamine (DDA). Flame-retardant polyamide 1210 (FRPA) is further prepared by copolymerizing the CDS, DDA, and sebacic acid (SEA). The test results show that the introduction of CDS can significantly improve the flame-retardant properties of FRPA. Specifically, the flame-retardant polyamide 1210 (FRPA-7) with 7 wt% CDS addition can reach V-0 grade according to UL-94 standard, accompanying limiting oxygen index value of 30.2% and tensile strength of 38.62 MPa. Compared with pure polyamide 1210, the peak heat release rate and total heat release rate of FRPA-7 reduce by 24.11% and 9.40%, respectively. This study provides a simple strategy to prepare flame-retardant polyamides with high flame retardancy and good mechanical properties, which are expected to show great potentials in future industrial applications.

About this research paper

What this paper is about

The thermal stability and reactivity of organophosphorus flame-retardants play a critical role in synthesizing copolymerized flame-retardant polyamides. Herein, this work successfully synthesizes a flame-retardant CEPPA-DDA salt (CDS) with both good thermal stability and high reactivity by reacting 2-carboxyethyl phenyl phosphonic acid (CEPPA) with 1,12-dodecanediamine (DDA). Flame-retardant polyamide 1210 (FRPA) is further prepared by copolymerizing the CDS, DDA, and sebacic acid (SEA). The test results show that the introduction of CDS can significantly improve the flame-retardant properties of FRPA. Specifically, the flame-retardant polyamide 1210 (FRPA-7) with 7 wt% CDS addition can reach V-0 grade according to UL-94 standard, accompanying limiting oxygen index value of 30.2% and tensile strength of 38.62 MPa. Compared with pure polyamide 1210, the peak heat release rate and total heat release rate of FRPA-7 reduce by 24.11% and 9.40%, respectively. This study provides a simple strategy to prepare flame-retardant polyamides with high flame retardancy and good mechanical properties, which are expected to show great potentials in future industrial applications.

Why it matters

OpenAlex reports 18 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

The thermal stability and reactivity of organophosphorus flame-retardants play a critical role in synthesizing copolymerized flame-retardant polyamides. Herein, this work successfully synthesizes a flame-retardant CEPPA-DDA salt (CDS) with both good thermal stability and high reactivity by reacting 2-carboxyethyl phenyl phosphonic acid (CEPPA) with 1,12-dodecanediamine (DDA). Flame-retardant polyamide 1210 (FRPA) is further prepared by copolymerizing the CDS, DDA, and sebacic acid (SEA). The test results show that the introduction of CDS can significantly improve the flame-retardant properties of FRPA. Specifically, the flame-retardant polyamide 1210 (FRPA-7) with 7 wt% CDS addition can reach V-0 grade according to UL-94 standard, accompanying limiting oxygen index value of 30.2% and tensile strength of 38.62 MPa. Compared with pure polyamide 1210, the peak heat release rate and total heat release rate of FRPA-7 reduce by 24.11% and 9.40%, respectively. This study provides a simple strategy to prepare flame-retardant polyamides with high flame retardancy and good mechanical properties, which are expected to show great potentials in future industrial applications.

Key concepts: Fire retardant, Polyamide, Limiting oxygen index, Thermal stability, Materials science, Ultimate tensile strength, Reactivity (psychology), Copolymer