2022•Journal of Engineering Materials and TechnologyRequires access

The Effect of Strain Rate on the Hydrogen Embrittlement Susceptibility of Aluminum 7075

Mehmet Furkan Baltacıoğlu, Barış Çetin, Burak Bal

Open publisher page 16 citations

Abstract

Abstract The effects of changing the strain rate regime from quasi-static to medium on hydrogen susceptibility of aluminum (Al) 7075 were investigated using tensile tests. Strain rates were selected as 1 s−1 and 10−3 s−1 and tensile tests were conducted on both hydrogen uncharged and hydrogen charged specimens at room temperature. Electrochemical hydrogen charging method was utilized and the diffusion length of hydrogen inside Al 7075 was modeled. Material characterizations were carried out by X-ray diffraction (XRD) and energy dispersive X-ray spectroscopy (EDX) and microstructural observations of hydrogen uncharged and hydrogen charged specimens were performed by scanning electron microscope (SEM). As opposed to earlier studies, hydrogen embrittlement (HE) was more pronounced at high strain rate cases. Moreover, hydrogen enhanced localized plasticity (HELP) was the more dominant hydrogen embrittlement mechanism at slower strain rate but coexistence of hydrogen enhanced localized plasticity and hydrogen enhanced decohesion was observed at a medium strain rate. Overall, the current findings shed light on the complicated hydrogen embrittlement behavior of Al 7075 and constitute an efficient guideline for the usage of Al 7075 that can be subject to different strain rate loadings in service.

About this research paper

What this paper is about

Abstract The effects of changing the strain rate regime from quasi-static to medium on hydrogen susceptibility of aluminum (Al) 7075 were investigated using tensile tests. Strain rates were selected as 1 s−1 and 10−3 s−1 and tensile tests were conducted on both hydrogen uncharged and hydrogen charged specimens at room temperature. Electrochemical hydrogen charging method was utilized and the diffusion length of hydrogen inside Al 7075 was modeled. Material characterizations were carried out by X-ray diffraction (XRD) and energy dispersive X-ray spectroscopy (EDX) and microstructural observations of hydrogen uncharged and hydrogen charged specimens were performed by scanning electron microscope (SEM). As opposed to earlier studies, hydrogen embrittlement (HE) was more pronounced at high strain rate cases. Moreover, hydrogen enhanced localized plasticity (HELP) was the more dominant hydrogen embrittlement mechanism at slower strain rate but coexistence of hydrogen enhanced localized plasticity and hydrogen enhanced decohesion was observed at a medium strain rate. Overall, the current findings shed light on the complicated hydrogen embrittlement behavior of Al 7075 and constitute an efficient guideline for the usage of Al 7075 that can be subject to different strain rate loadings in service.

Why it matters

OpenAlex reports 16 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Abstract The effects of changing the strain rate regime from quasi-static to medium on hydrogen susceptibility of aluminum (Al) 7075 were investigated using tensile tests. Strain rates were selected as 1 s−1 and 10−3 s−1 and tensile tests were conducted on both hydrogen uncharged and hydrogen charged specimens at room temperature. Electrochemical hydrogen charging method was utilized and the diffusion length of hydrogen inside Al 7075 was modeled. Material characterizations were carried out by X-ray diffraction (XRD) and energy dispersive X-ray spectroscopy (EDX) and microstructural observations of hydrogen uncharged and hydrogen charged specimens were performed by scanning electron microscope (SEM). As opposed to earlier studies, hydrogen embrittlement (HE) was more pronounced at high strain rate cases. Moreover, hydrogen enhanced localized plasticity (HELP) was the more dominant hydrogen embrittlement mechanism at slower strain rate but coexistence of hydrogen enhanced localized plasticity and hydrogen enhanced decohesion was observed at a medium strain rate. Overall, the current findings shed light on the complicated hydrogen embrittlement behavior of Al 7075 and constitute an efficient guideline for the usage of Al 7075 that can be subject to different strain rate loadings in service.

Key concepts: Hydrogen, Hydrogen embrittlement, Materials science, Strain rate, Ultimate tensile strength, Scanning electron microscope, Metallurgy, Embrittlement

Related papers

Back to paper searchBrowse research topicsOriginal source
The Effect of Strain Rate on the Hydrogen Embrittlement Susceptibility of Aluminum 7075 — Research Paper | ScholarLens